Williams Hayward Protective Coatings Aqua-Slip Waterborne Copolymer/Terpolymers is waterborne dispersions, emulsions or solution coatings. For use as a quick release coating for interiors of plastic pellet hoppers, coal cars, fly ash hoppers, refuse containers and recycle trucks. Polyethylene and /or Teflon extenders are used. The emulsion versions exhibit excellent acid and alkali resistance, while the dispersions and solution have dilute acid and alkali resistance.

Product Type: Mold Release Coating, Waterborne Coating

Features: Acid Resistant, Alkali Resistant, Freeze/Thaw Stability

Application Area: Containers, Truck

  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Features & Benefits

Labeling Claims

Applications & Uses

Application Area
Applications
  • Spray Technique: Cross coat - 50% overlap
  • Dry to Touch: 30-60 min.
  • Min. Recoat Time: 30-60 min.
  • Equipment Requirements: Airless/Air
  • Substrate: CRS, HRS,GALV,AL.
  • Surface Prep: SSPC-SP-6/Remove oil & grease
  • D.O.T.: Non-Flammable
  • Through dry: 10 - 12 hrs.

Properties

Typical Properties
ValueUnitsTest Method / Conditions
Filters60.0Mesh-
Application Temperaturemin. 50°F-
Application Temperaturemax. 85°F-
Steel Temperaturemax. 85°F-
Steel Temperaturemin. 50°F-
Pump Pressure1500 - 1800psi-
Required Dry Mils87.5 - 100micron-
Required Wet Mils150 - 200micron-
Solids by Volume50 - 54%-
Solvent TypeWater--
Tip Sizes6/19; 6/21’s--
V.O.C. (Dehydrated)0.6 - 1.20--
Viscosity40 - 50-J CUP

Technical Details & Test Data

Notes

* In coating application, the critical parameters are the relationship between surface temperature and dew point. The surface temperature must be a minimum of 5°F / -15°C above the dew point, with a minimum surface temperature of 50°F / 10°C.

** Aqua-Slip coatings will not lift or wrinkle when recoated. However, if the surface is to be recoated after 24 hours, it should be scuffed or lightly sanded to ensure proper inter-coat adhesion.

*** Aqua-Slip coatings made in Thermalbond polymer blends cannot be frozen. Certain Aqua-lust versions will pass 3-5 freeze thaw cycles. However, as with all waterborne coatings, they should be kept from freezing at all times.

  1. Dry times depend on humidity and total mils. The greater of either or both together will increase the time for the coating to dry. The reverse is also true, the lesser the humidity or mils decreases the time for the coating to dry. The use of air movement great assists in speeding up dry.
  2. Waterborne coatings will yield transfer efficiencies as high as 86-90% when proper tip sizes and pump pressures are used.