Multiflex® G 60 A 11 BT 13893 Thermoplastic Elastomer
Tear Strength: 23.0 - 23.0 kN/m
Strain at Break: 650.0 - 650.0 %
Multiflex® Automotive GT Range can be transformed between 190°C to 230°C. In this temperature range, materials are stable, above, thermal degradation occurs, resulting in yellowing and significant odor emanation. Multiflex® G 60 A 11 BT 13893 is designed for use in injection molding/extrusion
DuPont
Multiflex® G 62 A 21 B Z1631 N0052 (A) Thermoplastic Elastomer
Tear Strength: 37.0 - 37.0 kN/m
Strain at Break: 550.0 - 550.0 %
Compression Set (70 °C): 33.0 - 33.0 %
Multiflex® brand TES Automotive G Range are styrenics thermoplastic elastomers, designed for medium/high compression set applications. Compatibility with polyolefin enables bi-material parts (continuous process or cold insert).
DuPont
Multiflex® G 55 A 11 B Z1751 Thermoplastic Elastomer
Tear Strength: 24.0 - 24.0 kN/m
Multiflex™ G are thermoplastic elastomers based styrenic, combining soft touch, elasticity and compression set performances. Compatibility with polyolefin enables bi-material parts (continuous process or cold insert).
DuPont
Multiflex® G 75 A 520 205/09 10779 Thermoplastic Elastomer
Tear Strength: 35.0 - 35.0 kN/m
Multiflex® brand TES Automotive G Range are styrenics thermoplastic elastomers, designed for medium/high compression set applications. Compatibility with polyolefin enables bi-material parts (continuous process or cold insert).
DuPont
Multiflex® G 85 A 550 N0200 12121 Thermoplastic Elastomer
Tear Strength: 45.0 - 45.0 kN/m
Multiflex® Automotive G Range can be transformed between 190°C to 220–230°C. In this temperature range, materials are stable, above, thermal degradation occurs, resulting in yellowing and significant odor emanation.
DuPont
Multiflex® G 90 A 520
Polymer Name: Styrenic Thermoplastic Elastomer
Processing Methods: Injection Molding, Film Extrusion
Tear Strength: 48.0 - 48.0 kN/m
Strain at Break: 160.0 - 160.0 %
Multiflex® G 90 A 520 by DuPont is comprised of Styrenic Thermoplastic Elastomer. It is commonly used It is available in Pellets form.
DuPont
Multiflex® D 1047 BK0200 14688 Thermoplastic Elastomer
Density: 880.0 - 880.0 kg/m³
Strain at Break: 130.0 - 130.0 %
Flexural Modulus: 420.0 - 420.0 MPa
Multiflex® D 1047 BK0200 14688 Thermoplastic Elastomer by DuPont is comprised of Thermoplastic Polyolefin Elastomer. It is commonly used It is available in Pellets form.
DuPont
Multiflex® TES 2403 SI1 Black 27753 Thermoplastic Elastomer
Tear Strength: 76.0 - 76.0 kN/m
Strain at Break: 260.0 - 260.0 %
Multiflex® TES 2403 SI1 Black 27753 Thermoplastic Elastomer by DuPont is comprised of Styrenic Thermoplastic Elastomer. It is commonly used It is available in Pellets form.
DuPont
MULTIBASE™ MB50-001 MP
Function: Anti-Marring Agent, Processing Aid
Compatible Polymers & Resins: Polypropylenes (PP)
Processing Methods: Film Extrusion, Extrusion, Cable Extrusion, Injection Molding
Carrier: Resin-based, Polypropylenes (PP)
Features: Good Scratch Resistance, Good Processability, Fast Production Cycle
DuPont MB50-001 MP is a silicone masterbatch and has many benefits like improvement of scratch resistance, processing aid in melt phase, decreasing melt fracture, decreasing engine energy. Increasing out put for extrusion process
DuPont
Multiflex® TPO 7003 SW Natural Thermoplastic Elastomer
Density: 950.0 - 950.0 kg/m³
Strain at Break: 150.0 - 150.0 %
Flexural Modulus: 600.0 - 600.0 MPa
Multiflex® TPO 7003 SW Natural Thermoplastic Elastomer by DuPont is comprised of Thermoplastic Polyolefin Elastomer. It is commonly used It is available in Pellets form.
DuPont
Multiflex® G 90 A 21 B Z1668 N0042 Thermoplastic Elastomer
Tear Strength: 50.0 - 50.0 kN/m
Strain at Break: 400.0 - 400.0 %
Multiflex® brand are styrenics thermoplastic elastomers, designed for medium/high compression set applications. Compatibility with polyolefin enables bi-material parts (continuous process or cold insert). Multiflex® G 90 A 21 B Z1668 N0042 is designed for use in injection molding/extrusion.