company tower banner
Envalior Company Logo

Akulon® Ultraflow XG-FKGS6

1 of 199 products in this brand
Akulon® Ultraflow XG-FKGS6 is a high-performance polyamide 6 and polyamide 66 material trusted worldwide for applications in automotive, electronics, electrical, furniture, and packaging. In molded parts, it delivers an impressive blend of design simplicity and processing ease, along with exceptional mechanical properties across a wide temperature range and diverse conditions. For extrusion, it sets industry benchmarks, featuring remarkable strength, resilience, and ease of processing. This product boasts special features including 30% glass reinforcement, flame retardancy (halogen-free), and being best suited for injection molding.

Polymer Name: Polyamide 6 (PA 6)

Chemical Family: Polyamides

Reinforcement Material: Glass Fibers

Fillers Included: Glass Fiber

Processing Methods: Injection Molding, Injection Molding

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Chemical Family
Fillers Included
Polymer Name
Reinforcement Form
Reinforcement Material
Composite Materials Functions
Plastics & Elastomers Functions

Features & Benefits

Labeling Claims

Applications & Uses

Composites Processing Methods
Plastics & Elastomers Processing Methods
MCCB Housings Application Data

Details

Most grades are available with halogenfree flameretardancy, and in specific electro-gray color for housings. ForTii® Heat Deflection Temperature (HDT) of 305°C .

Benefits

  • Akulon® PA6 and ForTii® PA4T enable increased design flexibility and integrated functionality, facilitating smart assembly solutions
  • Akulon® PA6 and ForTii® PA4T allow for reliable solutions due to good dielectric aging performance at 150°C and high CTI values at 600 Volts
  • Akulon® PA6 and ForTii® PA4T allow for potential system cost reductions up to 15% ( wall thicknesses reduced leading to a volume reduction of up to 25%) compared to conventional materials
Industrial Control Gear Application Data

Details

Most grades are available with halogenfree flameretardancy, and in specific electro-gray color for housings. ForTii® Heat Deflection Temperature (HDT) of 305°C .

Benefits

  • Akulon® PA6 and ForTii® PA4T allow for reliable solutions due to good electrical and thermal endurance
  • Akulon® PA6 and ForTii® PA4T allow for more design freedom and/or potential system cost reductions due to part integration and thinner wall design and lower profiles possibilities, reduced cycle time with lower production losses
Contactors Application Data

Details

Most grades are available with halogenfree flameretardancy, and in specific electro-gray color for housings. Also Lasermarkable grades are available. ForTii® has a Heat Deflection Temperature (HDT) of 305°C .

Benefits

  • Akulon® PA6 and ForTii® PA4T allow for reliable solutions due to good electrical and thermal endurance
  • Akulon® PA6 and ForTii® PA4T allow for more design freedom and/or potential system cost reductions due to part integration and thinner wall design and lower profiles possibilities, reduced cycle time with lower production losses
EV Charging Plugs Application Data

Details

Envalior's portfolio of Akulon® PA6 and Arnite® PBT solutions for electric vehicle charging plugs can offer better surface appearance and mechanical performance without the need for expensive flame retardant additives. As electrical vehicle (EV) sales around the world continue to grow, Envalior is partnering with automakers and suppliers to develop advanced materials solutions to improve EV charging.

Benefits

  • UV resistance for better surface appearance
  • High impact strength and toughness to reduce normal wear and tear
  • Compliant with UL and IEC regulations
Residual Current Breaker with Overload Application Data

Details

Most grades are available with halogenfree flameretardancy, and in specific electro-gray color for housings.

Benefits

  • Akulon® PA6 and Arnite® PBT allow for reliable solutions due to excellent electrical (excellent short-circuit properties, including residual dielectric strength) and thermo-mechanical endurance compared to conventional materials
  • Akulon® PA6 and Arnite® PBT offer system cost down opportunities versus thermosets or other Engineering Materials
Potential Applications

Envalior's polyamide-based UD tapes with endless carbon or glass fiber reinforcements are viable, lightweight alternatives to metals in several applications. UD tapes, tape-based 2D fabrics and crossplies are used in structural and semi-structural applications, as well as in the selective reinforcement of injection molded parts.

 

DSM Engineering Materials Akulon CO-KGV4/A JN.00.86 Potential Applications - 1

A demonstration vehicle door panel made by JLR from carbon fiber-reinforced PA410, as well as fabric sheets woven from the same UD tape (EU-sponsored ENLIGHT project). The UD tape products were thermo-formed and glued to make the panel, which is 60% lighter than state- of-the-art, steel-based designs, while still fulfilling safety requirements. The full composite door consists of structural panels and a tape-wound side impact beam over an extruded, permanent mandrel.

 

DSM Engineering Materials Akulon CO-KGV4/A JN.00.86 Potential Applications - 2

Maxion Wheels and Envalior successfully manufactured and tested (Rim Rolling Fatigue) thin-walled hybrid, steelcomposite automotive wheel-rim reinforced with UD tape (tape-winding) made from glass fiber-reinforced PA410. The hybrid wheel-rim is 2Kg lighter and 30% more fatigue-resistant than state-ofthe- art, steel design, whilst inert to road salts and battery acids.

 

DSM Engineering Materials Akulon CO-KGV4/A JN.00.86 Potential Applications - 3

A vehicle central-floor module from carbon fiber-reinforced PA410 made by FCA (EU-sponsored ENLIGHT project). The UD tapes based ply-books were thermoformed to the final shape. The composite part is 18% lighter than state-of-the-art, steel-based designs, while still fulfilling safety requirements. The composite strength and dimensional stability are not affected by the E-coating process, a requirement of BIW parts.

Properties

Flame Rating
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Modulus11500 / 7500MPaISO 527-1/-2
Tensile Modulus (-40°C)12000 / -MPaISO 527-1/-2
Tensile Modulus (40°C)11000 / -MPaISO 527-1/-2
Tensile Modulus (100°C)5200 / -MPaISO 527-1/-2
Stress at Break140 / 90MPaISO 527-1/-2
Stress at Break (-40°C)190 / -MPaISO 527-1/-2
Stress at Break (100°C)70 / -MPaISO 527-1/-2
Strain at Break2.7 / 4%ISO 527-1/-2
Strain at Break (at -40°C)2.7 / -%ISO 527-1/-2
Flexural Modulus11200 / 7850MPaISO 178
Flexural Strength230 / 160MPaISO 178
Charpy Impact Strength (at +23°C)60 / 60kJ/m²ISO 179/1eU
Charpy Impact Strength (at -30°C)55 / 45kJ/m²ISO 179/1eU
Charpy Notched Impact Strength (at +23°C)9 / 12kJ/m²ISO 179/1eA
Charpy Notched Impact Strength (at -30°C)9.5 / 9kJ/m²ISO 179/1eA
Thermal Properties
ValueUnitsTest Method / Conditions
Temperature of Deflection Under Load (1.80 MPa)205 / *°CISO 75-1/-2
Burning Behaviour (at 1.5 mm Nominal Thickness)UL V-0 / *classIEC 60695-11-10
Burning Behaviour (at 3.0 mm Nominal Thickness)UL V-0 / *classIEC 60695-11-10
Burning Behaviour (at 0.75 mm Nominal Thickness)V-0 / *classIEC 60695-11-10
Burning Behaviour 5V (at 1.5 mm thickness h)UL 5VA / *classIEC 60695-11-20
Glow Wire Flammability Index (at thickness 1.6 / - mm)960 / -°CIEC 60695-2-12
Glow Wire Flammability Index (at thickness 0.8 / - mm)960 / -°CIEC 60695-2-12
Glow Wire Ignition Temperature (at thickness 1.6 / - mm)775 / -°CIEC 60695-2-13
Glow Wire Ignition Temperature (at thickness 1 / - mm)775 / -°CIEC 60695-2-13
Relative Temperature Index (Electrical, 0.75 / * mm)140 / *°CUL746B
Relative Temperature Index (Electrical, 3 / * mm)140 / *°CUL746B
Relative Temperature Index (with impact, 0.75 / * mm)110 / *°CUL746B
Relative Temperature Index (with impact, 3 / * mm)110 / *°CUL746B
Relative Temperature Index (without impact, 0.75 / * mm)140 / *°CUL746B
Relative Temperature Index (without impact, 3 / * mm)140 / *°CUL746B
Electrical Properties
ValueUnitsTest Method / Conditions
Electric Strength40 / -kV/mmIEC 60243-1
Comparative Tracking Index- / 600VIEC 60112
Other Properties
ValueUnitsTest Method / Conditions
Humidity Absorption1.7 / *%Sim. to ISO 62
Density1470 / -kg/m³ISO 1183
Rheological Properties
ValueUnitsTest Method / Conditions
Molding Shrinkage (parallel)0.2 / *%Sim. to ISO 294-4
Molding Shrinkage (normal)0.6 / *%Sim. to ISO 294-4

Regulatory & Compliance

Certifications & Compliance
Quality Standards

Technical Details & Test Data

Envalior's Automotive Weight Loss Factory

Extreme light weighting of automobiles is the most efficient technology for reducing emissions and enhancing mileage. The Envalior Weight Loss Factory utilizes unidirectional, continuous fiber-reinforced, thermoplastic tapes as the fundamental building block of such light weight composite materials.


Our strategy extends well beyond just manufacturing the composite tapes. We also develop and specify processes such as Automatic Tape Placement (ATP), tape winding and tape-insert over-molding. and the necessary computer aided engineering (CAE) for part design and manufacturing process specifications. Envalior is active in the industry in specifying and standardizing composite material testing and quality specifications.

 

UD tape processes

DSM Engineering Materials Akulon CO-KGV4/A JN.00.86 DSM's Automotive Weight Loss Factory

 

UD tape manfucaturing process

  1. Tape winding of parts with rotational symmetry (cylinders, tubes, box-beams etc.).
  2. Automatic Tape Laying (ATL) (panels, sheets, etc.)
    • ATL panels are thermoformed to net shape
    • ATL panels are over-molded with structural features (ribs, etc.).
  3. Hybrid metal-composite construction (composite patches glued to metal).

 

Technology and support

Design and CAE

  • FEM analyzes (static & high-strain)
  • Thermoforming and over-molding simulation
  • UD tape winding and simulation
  • Mold flow analyzes (injection-molding)

In-house macro & micro structural analysis of UD tapes

  • Material-modeling and micro-mechanics
  • Micro CT scans (void content, fiber-filament orientation, fiber-matrix adhesion, etc.)
  • SEM micrography
  • Tensile, flexural and impact testing.

Bonding

  • Composite to plastic
  • Composite to metal (with and without adhesives). 
Stress-Strain (cond.)

DSM Engineering Materials Akulon Ultraflow XG-FKGS6 Stress-Strain (cond.)

Chemical Resistance
Chemical TypeChemical NameResistance
OtherAcetaldehyde (40% by mass) at 23°Climited resistant, tests necessary to verify
OtherAcetamide (50% by mass) at 23°Climited resistant, tests necessary to verify
OtherAcetamide (50% by mass) at >140°Cnot resistant
OtherAcetic acid (10% by mass) at 100°Cnot resistant
OtherAcetic acid (10% by mass) at 23°Climited resistant, tests necessary to verify
OtherAcetic acid (95% by mass) at 23°Cnot resistant
KetonesAcetone at 23°Cresistant
OtherAcetophenone at 23°Cresistant
OtherAcetyl chloride at 23°Cnot resistant
OtherAcetylene at 23°Cresistant
OtherAcrylic acid at 23°Cnot resistant
OtherAliphatic amines at 23°Cresistant
OtherAliphatic hydrocarbons at 23°Cresistant
OtherAlkylbenzenes at 23°Cresistant
OtherAllyl alcohol at 23°Climited resistant, tests necessary to verify
OtherAluminum acetate (saturated) at 23°Cresistant
OtherAluminum chloride (10% by mass) at 23°Cresistant
OtherAluminum hydroxide (saturated) at 23°Cresistant
OtherAluminum salts of mineral acids (saturated) at 23°Climited resistant, tests necessary to verify
OtherAluminum trichloride (10% by mass) at 23°Cresistant
OtherAmino acids (saturated) at 23°Cresistant
OtherAmmonia at 23°Cresistant
OtherAmmonium chloride (35% by mass) at 100°Climited resistant, tests necessary to verify
OtherAmmonium chloride (35% by mass) at 23°Cresistant
OtherAmmonium salts of mineral acids (10% by mass) at 23°Cresistant
OtherAmmonium salts of mineral acids (10% by mass) at 50°Climited resistant, tests necessary to verify
OtherAmmonium thiocyanate (saturated) at 23°Cresistant
OtherAmyl acetate at 100°Cnot resistant
OtherAmyl acetate at 23°Cresistant
OtherAmyl alcohol at 23°Cresistant
OtherAniline at 23°Cnot resistant
OtherAnodizing liquid (HNO3/H2SO4) at 23°Climited resistant, tests necessary to verify
OtherAntimony trichoride (saturated) at 23°Cnot resistant
OtherAqua Regia (HCl/HNO3) at 23°Cnot resistant
OtherAromatic hydrocarbons at 23°Cresistant
OtherBariumsalts of mineral acids at 23°Climited resistant, tests necessary to verify
OtherBenzaldehyde at 23°Climited resistant, tests necessary to verify
OtherBenzene at 23°Cresistant
OtherBenzene at 80°Cresistant
OtherBenzoic acid (20% by mass) at 23°Climited resistant, tests necessary to verify
OtherBenzoic acid (saturated) at 23°Cnot resistant
OtherBenzyl alcohol at 23°Climited resistant, tests necessary to verify
OtherBeverages at 23°Cresistant
OtherBleaching agent (NaOCl) at 23°Cnot resistant
OtherBoric acid (10% by mass) at 23°Climited resistant, tests necessary to verify
OtherBoron trifluoride at 23°Cnot resistant
OtherBrake fluids (DOT 3/4) at 23°Climited resistant, tests necessary to verify
OtherBromine water (saturated) at 23°Cnot resistant
OtherBromochlorodifluoromethane at 23°Cresistant
OtherBromotrifluoromethane at 23°Cresistant
OtherButadiene at 23°Cresistant
OtherButane at 23°Cresistant
OtherButanediols at 23°Cresistant
OtherButanediols at >140°Climited resistant, tests necessary to verify
OtherButanols at 23°Cresistant
OtherButene glycol at 23°Cresistant
OtherButene glycol at >160°Climited resistant, tests necessary to verify
OtherButene-1 at 23°Cresistant
OtherButter at 23°Cresistant
OtherButyl acetate at 23°Cresistant
OtherButyl acrylate at 23°Cresistant
OtherButyl glycolate at 23°Cresistant
OtherButyl phthalate at 23°Cresistant
OtherButyric acid (20% by mass) at 23°Climited resistant, tests necessary to verify
OtherButyrolactone at 23°Cresistant
OtherButyrolactone at >90°Climited resistant, tests necessary to verify
OtherCalcium chloride (10% by mass) at 100°Climited resistant, tests necessary to verify
OtherCalcium chloride (10% by mass) at 23°Cresistant
OtherCalcium chloride (alcoholic) (20% by mass) at 23°Climited resistant, tests necessary to verify
OtherCalcium chloride (saturated) at 100°Cnot resistant
OtherCalcium chloride (saturated) at 23°Cresistant
OtherCalcium chloride (saturated) at 60°Climited resistant, tests necessary to verify
OtherCalcium hydroxide (saturated) at 23°Cresistant
OtherCalcium hypochloride (saturated) at 23°Cnot resistant
OtherCamphor (alcoholic) (50% by mass) at 23°Cresistant
OtherCaprolactam (50% by mass) at 23°Cresistant
OtherCaprolactam (50% by mass) at >150°Climited resistant, tests necessary to verify
OtherCarbon disulfide at 23°Cresistant
OtherCarbon disulfide at 60°Cnot resistant
OtherCarbon tetrachloride at 23°Cresistant
OtherCasein at 23°Cresistant
OtherChloral hydrate at 23°Cnot resistant
OtherChloramines (10% by mass) at 23°Cnot resistant
OtherChlorinated biphenyls at 80°Climited resistant, tests necessary to verify
OtherChlorine water at 23°Cnot resistant
OtherChloroacetic acid (10% by mass) at 23°Cnot resistant
OtherChlorobenzene at 23°Cresistant
OtherChlorobenzene at 50°Cresistant
OtherChlorobromomethane at 23°Climited resistant, tests necessary to verify
OtherChlorodifluoroethane at 23°Cresistant
OtherChlorodifluoromethane at 23°Cresistant
OtherChlorofluoroethylene at 23°Cresistant
OtherChloroform at 23°Cnot resistant
OtherChlorosulfonic acid (10% by mass) at 23°Cnot resistant
OtherChromic acid (1% by mass) at 23°Climited resistant, tests necessary to verify
OtherChromic acid (10% by mass) at 23°Cnot resistant
OtherChromyl chloride at 23°Cnot resistant
Othercis-2-butene at 23°Cresistant
OtherCitric acid (10% by mass) at 23°Cresistant
OtherCitric acid (20% by mass) at 80°Climited resistant, tests necessary to verify
OtherCobalt salt (20% by mass) at 23°Climited resistant, tests necessary to verify
OtherCopper sulfate (10% by mass) at 23°Cresistant
OtherCopper(II) salt (10% by mass) at 23°Climited resistant, tests necessary to verify
OtherCresols at 23°Cnot resistant
OtherCycloalcohols (incl their esters) at 23°Cresistant
OtherCycloalkanes at 23°Cresistant
OtherCycloalkanones at 23°Cresistant
OtherCyclohexanol at 23°Climited resistant, tests necessary to verify
OtherDecalin at 23°Cresistant
OtherDeveloper (photografic) at 23°Cresistant
OtherDibutyl phthalate at 23°Cresistant
OtherDibutyl phthalate at 60°Cresistant
OtherDichlorobenzene at 23°Cresistant
OtherDichloroethane at 23°Cresistant
OtherDichloroethylene at 23°Cresistant
OtherDichlorofluoromethane at 23°Cresistant
OtherDichlorotetrafluoroethane at 23°Cresistant
EthersDiethyl ether at 23°Cresistant
OtherDiethylene glycol at 23°Cresistant
OtherDiethylene glycol at >140°Cnot resistant
OtherDifluoromethane at 23°Cresistant
OtherDimethyl acetamide at 23°Cresistant
OtherDimethyl acetamide at >150°Cnot resistant
OtherDimethyl ether at 23°Cresistant
OtherDimethylamine at 23°Cresistant
OtherDimethylformamide at 23°Cresistant
OtherDimethylformamide at 90°Climited resistant, tests necessary to verify
OtherDimethylsilane at 23°Cresistant
OtherDimethylsulfoxide at 125°Cnot resistant
OtherDimethylsulfoxide at 23°Cresistant
OtherDioctyl phtalate at 23°Cresistant
OtherDioxan at 23°Cresistant
OtherDioxan at 60°Cresistant
OtherDiphenyl ether at 80°Cresistant
OtherDipropyl ether at 23°Cresistant
OtherEdible fats waxes and oils at 100°Cresistant
OtherElectroplating bath (acidic) at 23°Cnot resistant
OtherElectroplating bath (alkali) at 23°Cresistant
OtherEthane at 23°Cresistant
AlcoholsEthanol at 23°Cresistant
OtherEthyl Acetate at 23°Cresistant
OtherEthyl chloride at 23°Cresistant
OtherEthylene at 23°Cresistant
OtherEthylene carbonate at 100°Cnot resistant
OtherEthylene carbonate at 50°Cresistant
OtherEthylene chlorohydrin at 23°Climited resistant, tests necessary to verify
OtherEthylene glycol at 100°Cnot resistant
OtherEthylene glycol at 23°Cresistant
OtherEthylene oxide at 23°Cresistant
OtherEthylene oxide at >80°Cnot resistant
OtherEthylenediamine at 23°Cresistant
OtherFatty acids at 23°Cresistant
OtherFatty alcohols at 23°Cresistant
OtherFerric chloride (2,5% by mass) at 100°Cnot resistant
OtherFerric chloride (2,5% by mass) at 23°Climited resistant, tests necessary to verify
OtherFixer (photografic) at 23°Cresistant
OtherFluorinated hydrocarbons at 70°Cresistant
OtherFluorine at 23°Cnot resistant
OtherFormaldehyde (30% by mass) at 23°Cresistant
OtherFormamide at 23°Cresistant
OtherFormamide at >150°Cnot resistant
OtherFormic acid (10% by mass) at 23°Cnot resistant
OtherFormic acid (10% by mass) at 50°Cnot resistant
OtherFruit juices at 23°Cresistant
OtherFuel; Diesel at 85°Cresistant
OtherFuel; FAM 1A at 23°Cresistant
OtherFuel; FAM 2A at 23°Cresistant
OtherFuel; Gasoline at 85°Cresistant
OtherFurfural at 23°Cresistant
OtherFurfuryl alcohol at 23°Cresistant
OtherGlycerol at 170°Cnot resistant
OtherGlycerol at 23°Cresistant
OtherGlycolic acid (30% by mass) at 23°Cnot resistant
OtherGlycols at 23°Cresistant
OtherGrease (based on ester oils) at <100°Climited resistant, tests necessary to verify
OtherGrease (based on metal soaps) at <100°Cresistant
OtherGrease (based on polyphenylester) at <100°Cresistant
OtherHardening oils at 23°Cresistant
OtherHeating oils at 23°Cresistant
OtherHeptane at 23°Cresistant
OtherHexachlorobenzene at 80°Cresistant
OtherHexachloroethane at 23°Cresistant
OtherHexafluoroisopropanol at 23°Cnot resistant
OtherHexane at 23°Cresistant
OtherHydraulic fluids at 100°Cresistant
OtherHydrobromic acid (10% by mass) at 23°Cnot resistant
OtherHydrochloric acid (10% by mass) at 23°Cnot resistant
OtherHydrochloric acid (20% by mass) at 23°Cnot resistant
OtherHydrochloric acid (conc.% by mass) at 23°Cnot resistant
OtherHydrofluoric acid (40% by mass) at 23°Cnot resistant
OtherHydrofluoric acid (5% by mass) at 23°Cnot resistant
OtherHydrogen at 23°Cresistant
OtherHydrogen peroxide (0.5% by mass) at 23°Climited resistant, tests necessary to verify
OtherHydrogen peroxide (1% by mass) at 23°Cnot resistant
OtherHydrogen peroxide (3% by mass) at 23°Cnot resistant
OtherHydrogen peroxide (30% by mass) at 23°Cnot resistant
OtherHydrogen sulfide (10% by mass) at 23°Climited resistant, tests necessary to verify
OtherHydroiodic acid at 23°Cnot resistant
OtherHydroquinone (5% by mass) at 23°Cnot resistant
OtherImpregnating oils at 23°Cresistant
OtherInk at 23°Cresistant
OtherIodine (alcoholic) at 23°Cnot resistant
OtherIron(III)chloride (acidic) (10% by mass) at 23°Cnot resistant
OtherIron(III)chloride (neutral) (10% by mass) at 23°Cresistant
OtherIron(III)chloride (saturated) at 23°Cnot resistant
OtherIron(III)thiocyanate (10% by mass) at 23°Climited resistant, tests necessary to verify
OtherIsocyanates (aromatic) at 23°Cresistant
OtherIsooctane at 80°Cresistant
OtherIsopropanol at 23°Cresistant
OtherIsopropanol at 60°Cresistant
OtherKetones (aliphatic) at 23°Cresistant
OtherLactic acid at 10°Cresistant
OtherLactic acid at 90°Cnot resistant
OtherLead acetate (10% by mass) at 23°Cresistant
OtherLinseed oil at 23°Cresistant
OtherLithium bromide (10% by mass) at 23°Climited resistant, tests necessary to verify
OtherLithium chloride (20% by mass) at 23°Cnot resistant
OtherLithium hydroxide (10% by mass) at 23°Cresistant
OtherLithium hydroxide (10% by mass) at 80°Cnot resistant
OtherLubricating oil (gear) at <130°Cresistant
OtherLubricating oil (hydraulics) at <130°Cresistant
OtherLubricating oil (transformers) at <130°Cresistant
OtherMagnesium hydroxide (10% by mass) at 23°Cresistant
OtherMagnesium salts (10% by mass) at 23°Cresistant
OtherMaleic acid (25% by mass) at 23°Climited resistant, tests necessary to verify
OtherMaleic acid (saturated) at 23°Cresistant
OtherManganese salts (10% by mass) at 23°Cresistant
OtherMercury at 23°Cresistant
OtherMercury(II)chloride (saturated) at 23°Cnot resistant
OtherMethane at 23°Cresistant
AlcoholsMethanol at 23°Cresistant
OtherMethyl acetate at 23°Cresistant
OtherMethyl chloride at 23°Cresistant
OtherMethyl ethyl ketone at 23°Cresistant
OtherMethyl formate at 23°Cresistant
OtherMethyl glycol at 23°Cresistant
OtherMethylamine at 23°Cresistant
OtherMethylaniline at 23°Cresistant
OtherMethylbromide at 23°Cresistant
OtherMethylene chloride at 23°Climited resistant, tests necessary to verify
OtherMethylpyrrolidone at 23°Cresistant
OtherMilk at 23°Cresistant
Othern-Butyl ether at 23°Cresistant
Othern-Butyl glycol at 23°Cresistant
OtherNaphtha at 23°Cresistant
OtherNaphthalene at 23°Cresistant
OtherNaphthalenesulfonic acids at 23°Cnot resistant
OtherNaphthenic acids at 23°Cresistant
OtherNaphthols at 23°Cnot resistant
OtherNickel nitrate (10% by mass) at 23°Climited resistant, tests necessary to verify
OtherNickel salts (10% by mass) at 23°Cresistant
OtherNitric acid (10% by mass) at 23°Cnot resistant
OtherNitric acid (2% by mass) at 23°Cnot resistant
OtherNitric acid (20% by mass) at 23°Cnot resistant
OtherNitric acid (conc.% by mass) at 23°Cnot resistant
OtherNitrobenzene at >100°Cnot resistant
OtherNitrocellulose lacquers (non-alcoholic) at 23°Cresistant
OtherNitrotoluene at >100°Cnot resistant
OtherNitrous oxide at 23°Cresistant
OtherOctane at 23°Cresistant
OtherOctene at 23°Cresistant
OtherOil (Shell 10W40) at 23°Cresistant
OtherOil (transformers, switchgear) at 50°Cresistant
OtherOils (vegatable, mineral, ethereal) at 23°Cresistant
OtherOleic acid at 23°Cresistant
OtherOleum (H2SO4+SO3) at 23°Cnot resistant
OtherOxalic acid (10% by mass) at 80°Cnot resistant
OtherOzone at 23°Cnot resistant
OtherPaint solvents at 23°Cresistant
OtherPalmatic acid at 80°Cresistant
OtherParaffin at 23°Cresistant
OtherPeracetic acid at 23°Cnot resistant
OtherPerchloric acid (10% by mass) at 23°Cnot resistant
OtherPetroleum at 23°Cresistant
OtherPetroleum ether and solvents at 80°Cresistant
OtherPhenol (conc.% by mass) at 23°Cnot resistant
OtherPhenol at >40°Cnot resistant
OtherPhenyl ether at 23°Cnot resistant
OtherPhenyl ethyl alcohol at >160°Cnot resistant
OtherPhosphate sol. (neutral, alkaline) (10% by mass) at 23°Cresistant
OtherPhosphine at 23°Cresistant
OtherPhosphoric acid (10% by mass) at 23°Cnot resistant
OtherPhosphoric acid (conc.% by mass) at 23°Cnot resistant
OtherPolyols at 23°Cresistant
OtherPotassium chloride (10% by mass) at 23°Cresistant
OtherPotassium chloride (10% by mass) at 70°Cresistant
OtherPotassium nitrate (10% by mass) at 23°Cresistant
OtherPotassium permanganate (1% by mass) at 23°Cnot resistant
OtherPotassium thiocyanate (saturated) at 23°Cnot resistant
OtherPropane at 23°Cresistant
OtherPropanol at 23°Cresistant
OtherPropanol at >100°Cnot resistant
OtherPropene at 23°Cresistant
OtherPropionic acid (5% by mass) at 23°Cresistant
OtherPropionic acid (50% by mass) at 23°Cnot resistant
OtherPyridine at 23°Cresistant
OtherPyrocatechol at 23°Cnot resistant
OtherPyrrolidone at 23°Cresistant
OtherRainwater (acidic) at 23°Cresistant
OtherRefrigerator oil at 23°Cresistant
OtherResorcinol (alcoholic) (50% by mass) at 23°Cnot resistant
OtherRoad salts at 23°Cresistant
OtherSalicylic acid (saturated) at 23°Cresistant
OtherSeawater at 23°Cresistant
OtherSilane at 23°Cresistant
OtherSilicone oils at <80°Cresistant
OtherSilver nitrate (10% by mass) at 23°Cresistant
OtherSoap solution (10% by mass) at 80°Cresistant
OtherSodium bichromate (10% by mass) at 23°Cresistant
OtherSodium bichromate (5% by mass) at 23°Cresistant
OtherSodium carbonate (10% by mass) at 23°Cresistant
OtherSodium chlorate (10% by mass) at 23°Cresistant
OtherSodium chloride (10% by mass) at 23°Cresistant
OtherSodium chloride (saturated) at 23°Cresistant
OtherSodium cyanide (10% by mass) at 23°Cresistant
OtherSodium dichromate (10% by mass) at 23°Cresistant
OtherSodium dodecylbenzenesulfonate at 23°Cresistant
OtherSodium hydrogen carbonate (10% by mass) at 23°Cresistant
OtherSodium hydrogen sulfate (10% by mass) at 23°Cresistant
OtherSodium hydrogen sulfite (10% by mass) at 23°Cresistant
OtherSodium hydroxide (10% by mass) at 23°Cresistant
OtherSodium hydroxide (10% by mass) at 80°Cnot resistant
OtherSodium hypophosphite (10% by mass) at 23°Cresistant
OtherSodium lauryl sulfate (30% by mass) at 23°Cresistant
OtherSodium lignosulfonate at 23°Cresistant
OtherSodium nitrilotriacetate (10% by mass) at 23°Cresistant
OtherSodium oleate at 23°Cresistant
OtherSodium pentachlorophenolate at 23°Cresistant
OtherSodium pyrosulfite (10% by mass) at 23°Cresistant
OtherSodium salts (nitrate, sulfate) (10% by mass) at 23°Cresistant
OtherSoldering fluid at 23°Cnot resistant
OtherStearate at 23°Cresistant
OtherStearic acid at 23°Cresistant
OtherStyrene at 80°Cresistant
OtherSulfonates (10% by mass) at 23°Cresistant
OtherSulfur at 23°Cresistant
OtherSulfur dioxide (dry) at 23°Cresistant
OtherSulfur hexafluoride at 23°Cresistant
OtherSulfuric acid (2% by mass) at 23°Cnot resistant
OtherSulfuric acid (30% by mass) at 23°Cnot resistant
OtherSulfuric acid (50% by mass) at 23°Cnot resistant
OtherSulfuric acid (conc.% by mass) at 23°Cnot resistant
OtherTartaric acid (10% by mass) at 23°Cresistant
OtherTetrachloroethylene at 80°Cnot resistant
OtherTetrachloromethane at 23°Cresistant
OtherTetrafluoromethane at 23°Cresistant
OtherTetrafluoropropanol at 23°Cnot resistant
OtherTetrahydrofuran at 23°Cresistant
OtherTetralin at 23°Cresistant
OtherTetramethylenesulfone at 23°Cresistant
OtherToluene at 100°Cresistant
HydrocarbonsToluene at 23°Cresistant
OtherTransformer oil at 23°Cresistant
OtherTrichloroacetic acid (50% by mass) at 23°Cnot resistant
OtherTrichloroethane at 45°Cresistant
OtherTrichloroethanol at 23°Cnot resistant
OtherTrichloroethylene at >40°Cnot resistant
OtherTrichlorotrifluoroethane at 23°Cresistant
OtherTrietanolamine at 23°Cresistant
OtherTrifluoroethanol at 23°Cnot resistant
OtherTrimethylamine at 23°Cresistant
OtherTurpentine oil at 23°Cresistant
OtherTurpentine substitute at 23°Cresistant
OtherUranium fluoride at 23°Cnot resistant
OtherUrea (20% by mass) at 23°Cresistant
OtherUric acid (20% by mass) at 23°Cresistant
OtherUrine at 23°Cresistant
OtherVaseline (acid free) at 23°Cresistant
OtherVinyl bromide at 23°Cresistant
OtherVinyl chloride at 23°Cresistant
OtherVinyl fluoride at 23°Cresistant
OtherWater (chlorinated) at 80°Cresistant
OtherWater at 23°Cresistant
OtherWax at 80°Cresistant
OtherXylene at 100°Cresistant
OtherXylene at 23°Cresistant
OtherYeast at 23°Cresistant
OtherZinc bromide (30% by mass) at 23°Cnot resistant
OtherZinc chloride (10% by mass) at 23°Climited resistant, tests necessary to verify
OtherZinc chloride (37% by mass) at 23°Cnot resistant
OtherZinc chloride at 23°Cresistant
OtherZinc iodide (30% by mass) at 23°Cnot resistant
OtherZinc nitrate (30% by mass) at 23°Cnot resistant
OtherZinc thiocyanate (30% by mass) at 23°Cnot resistant
OtherZinc(II)salts of mineral acids (10% by mass) at 23°Climited resistant, tests necessary to verify
Stress-Strain (dry)

DSM Engineering Materials Akulon Ultraflow XG-FKGS6 Stress-Strain (dry)

Packaging & Availability