Goldsmith & Eggleton Company Logo
G&E 254 is produced from feedstocks carefully selected for uniform viscosity, ethylene propylene ratio, and 3rd monomer. The feedstocks are chosen to produce a blended EPDM Polymer which has a medium ethylene content, medium diene content, and low mooney. G&E Blended EPDM 254 can be blended with prime EPDM polymers to reduce compound costs in extruded, calendered and molded applications.

Polymer Name: Ethylene Propylene Diene Terpolymer (EPDM)

Processing Methods: Calendering, Extrusion, Injection Molding

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Technologies

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Physical Form
Typical Properties
ValueUnitsTest Method / Conditions
MOONEY VISCOSITY (ML 1+4 at 125°C)29 ±10
Raw Polymer Specific Gravity0.86
Volatile Mattermax. 1.0 wt%
Ethylene Content57 ± 5wt%
ENB ContentMediumwt%

Packaging & Availability

Packaging Type
Packaging

55 lb. (25 kg.) bales are wrapped in low melt polyethylene film and are packaged in Returnable Metal Boxes, weighing approximately 2,600 lbs. (1.18 MT) each