company tower banner
Green Dot Bioplastics Inc Company Logo

Terratek® WC100299

1 of 39 products in this brand

Polymer Name: Thermoplastic (unspecified)

Reinforcement Material: Wood Fiber

Labeling Claims: Bio-based, Biodegradable, Sustainable

Processing Methods: Extrusion, Injection Molding, Profile Extrusion

Density: 1450.0 - 1450.0 kg/m³

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Reinforcement Material
Composite Materials Functions
Plastics & Elastomers Functions

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods
General Processing Recommendations

Green Dot’s Terratek® WC100299 resin needs to be dried before processing if the moisture is above 0.5%.  Resin will dry quickly at 150°F in a desiccant dryer.  Avoid prolonged resin exposure to air during molding or storage as the material can pick up moisture.

For best molding results, larger gates and runners are recommended. The injection pressure required to fill the mold is much higher than typical injection molding grade plastics.  Typical injection molding temperatures are listed below, these are only a guide and may need to be changed based on the particular application :

Rear 350°F to 360°F
Middle 350°F to 360°F
Front 360°F to 375°F
Nozzle 360°F to 375°F
Mold 60°F to 170°F

The melt temperature of the resin should remain below 400°F to prevent the material from discoloring and having a burnt odor.

Properties

Physical Form
Typical Properties
ValueUnitsTest Method / Conditions
Specific Gravity1.45ISO 1183-1
Moisturemax. 1%
Tensile Stressmax. 5500psiASTM D638
Tensile Modulus824000psi
Flexural Modulus683000psiASTM D790
Notched Impact Strength1.1ft lb/inASTM D256

Packaging & Availability

Packaging Type
Packaging

Terratek® WC100299 resin is typically packaged in a sealed plastic-lined Gaylord at 1,500 lbs/Gaylord.

Storage & Handling

Storing

The product should be stored in a cool, dry, and sanitary area to achieve maximum stability.