- HD-6000 DMM crosslinked with water-dispersible isocyanates may be spray applied using single-component equipment.
- The workable potlife is approximately 3 hours at the suggested crosslinker ratio of 2.0 to 1.0 NCO / OH.
Properties
- Physical Form
- Physical Properties
- Mechanical Properties (TPE)
Value | Units | Test Method / Conditions | |
Solids | 34 - 36 | % | — |
Viscosity | 50 - 500 | cps | — |
pH | 7.5 - 10.0 | — | — |
Density | 8.8 | lbs/gal | — |
VOC Content | 70 | gm/l | — |
OH Equivalent Weight (as supplied) | 3100 | g/l | — |
Sward Hardness | 44 | — | — |
Value | Units | Test Method / Conditions | |
Elongation | 230 | % | Tested at 20 inches/minute |
Tensile Strength | 7000 | psi | Tested at 20 inches/minute |
100% Modulus | 4850 | psi | Tested at 20 inches/minute |
200% Modulus | 6800 | psi | Tested at 20 inches/minute |
Technical Details & Test Data
- Drying
- HD-6000 DMM, crosslinked with a water dispersible isocyanate, will dry to a hard film in 30 minutes at ambient room temperature (65 -+ 70°F) and humidity (RH 50%).
- Ultimate cured properties will take 3 -5 days to develop.
- If heat is available, the ultimate properties can be attained in shorter time.
- Typical oven drying temperatures and dwell times for aqueous coatings are sufficient to produce optimal film properties.