company tower banner
JSC Sterlitamak Petrochemical Plant Company Logo

JSC Sterlitamak Petrochemical Plant SKS-30 ARKM-27 / SBR-1723

JSC Sterlitamak Petrochemical Plant SKS-30 ARKM-27 / SBR-1723 is a styrene and butadiene copolymer obtained by cold polymerization with the use of mixture of rosin and fatty acids soaps, filled with TDAE-type aromatic oil and stabilized by staining antioxidant.

Polymer Name: Styrene Butadiene Copolymer

Additives Included: Antioxidant

End Uses: Tires

Features: Cold Polymerized

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Technologies

Features & Benefits

Materials Features

Applications & Uses

Plastics & Elastomers End Uses
Applications

It is widely used in tire, industrial rubber and other industries.

Properties

Color
Appearance
Briquettes (Bales)
Typical Properties
ValueUnitsTest Method / Conditions
ML1.6-2.3dNmASTM D 5289
t'506.5-10.5minASTM D 5289
t'9015-18.5minASTM D 5289
ts13.5-6.5ASTM D 5289
МН12.6-16.5dNmASTM D 5289
Antioxidant Content (Agidol-2)0.8-1.5%Method of Supplier
Antioxidant Content (VS-1)0.3-0.7%Method of Supplier
Ash Contentmax. 0.6%ASTM D 5667 (Part A)
Bound Styrene Content22-25%ASTM D 5775
Mooney Viscosity ML 1+4 (100°C)47-57ASTM D 1646 (Para. 7.2.2)
Oil (TDAE) Content26-29%ASTM D 5774
Organic acid Content4.0-5.6%ASTM D 5774
Organic Acids Soaps Contentmax. 0.3%ASTM D 5774
Viscosity Spread within a Batchmax. 6units
Volatile matter Content (1 hour)max. 0.6%ASTM D 5668 (Method C)
Weight30.0+/-1.0kg

Regulatory & Compliance

Certifications & Compliance

Technical Details & Test Data

Rubber Mix Recipe and Measurement Conditions

Preparation of rubber mixes is carried out in accordance with ASTMD 3185 recipe 1А, mixing - according to method A. Mixing mills are prepared according to ASTM D 3182. Rheometric properties are determined according to ASTM D 5289 using an MDR 2000 rheometer (flow meter). Wait time for rubber mix before testing is 2-6 hours.

Parameters Standard
Rubber mix recipe in parts by weight acc. to ASTM D 3185, recipe 1А:
- Rubber 100
- Zinc oxide 3
- IRB 7 (N330) carbon black 50.00
- Sulfur 1.75
- Stearic acid 1
- TBBS (N-tert-Butyl-2- benzothiazolesulfenamide) 1.00
Rheometer MDR 2000, measurement conditions:
- Temperature, оС 160
- Duration, min 30
- Oscillation amplitude, deg. +/-0.5
- Oscillation frequency, Hz 1.7

Packaging & Availability

Packaging Type
Packing

Rubber briquettes (bales) are packaged in marked PE film (thickness of 0.05 +/- 0.01 mm, melting temperature of 108-112оС), then – in plastic box pallets of 450kg or in plywood containers of 1,080kg, or metal containers of 1,260kg.

Transportation

Rubber is transported by all types of transport in covered transporting means in accordance to all rules of cargo’s transportation standing at transport of this form.

Storage & Handling

Storage

At a temperature not exceeding 30оС, in dry place free from direct sunlight.

Guaranteed Shelf Life

1 (one) year from the manufacture date. After the expiration of the guaranteed shelf life, the rubber can be used for its intended purpose after confirmation of its conformity to the requirements of this product specification