Knowde Enhanced TDS
Identification & Functionality
- Polymer Name
- Plastics & Elastomers Functions
- Technologies
- Product Families
Features & Benefits
- Materials Features
- Features
- Available in thicknesses from 1.00mm (0.040”) and up and in eight distinctive textures and custom colors
- Meets the requirements of the Federal Aviation Administration FAR 25.853 (a) in all thicknesses for vertical burn
- Heat distortion temperature (HDT) is 85°C (185°F) unannealed at 1.8 MPa (264 psi) and a high 90°C (195°F) after annealing
- Excellent forming properties, uniform wall thickness and crisp detail
- Easy machining and fabricating using conventional methods and equipment
Applications & Uses
- Applications
- Plastics & Elastomers Processing Methods
- Applications
- Aircraft Interiors
- Equipment Housings
Properties
- Mechanical Properties
- Physical Properties
- Typical Properties
- Thermal Properties
- Flammability
Value | Units | Test Method / Conditions | |
Bearing Strength | max. 198 | MPa | ASTM D953 |
Bearing Strength (4% Defelection) | 19.3 | MPa | ASTM D953 |
Flexural Modulus | 2241 | MPa | ASTM D790 |
Flexural Strength | 66 | MPa | ASTM D790 |
Notched Izod Impact | 267 | J/m | ASTM D256 |
Tensile Strength | 44 | MPa | ASTM D638 |
Value | Units | Test Method / Conditions | |
Rockwell Hardness (R-Scale) | 104 | — | ASTM D785 |
Specific Gravity | 1.33 - 1.37 | — | ASTM D792 |
Value | Units | Test Method / Conditions | |
Rockwell Hardness | 104 | Scale R | ASTM D785 |
Value | Units | Test Method / Conditions | |
Heat Deflection Temperature (264 psi (1.8 MPa) Annealed) | 85 | °C | ASTM D648 |
Heat Deflection Temperature (264 psi (1.8 MPa) Annealed) | 90.6 | °C | ASTM D648 |
Value | Units | Test Method / Conditions | |
Vertical Burn (12-second) | Pass | — | FAR 25.853(a)(i) |
Vertical Burn (60-second) | Pass | — | FAR 25.853(a)(i) |