Nexceris Lanthanum Strontium Cobalt Ink

Nexceris Lanthanum Strontium Cobalt Ink is made using our quality LSC powder to provide an excellent cathode ink. It can be used to fabricate your own cells, and can be used to enhance contact of your solid oxide fuel cell to the test manifold.

Application Area: Battery Packs, Cathode, Electrical Components

Compatible Substrates & Surfaces: Ceramic, Metal

Features: Good Adhesion, Good Electrical Properties

Application Method: Screen Coating

Chemical Family: Cobalt & Cobalt Compounds, Lanthanum Compounds, Strontium & Strontium Compounds

Safety Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Product Type
Molecular formula
(La₀.₈₀Sr₀.₂₀)₀.₉₅CoO₃₋ₓ

Features & Benefits

Ready-to-Use Product Features

Applications & Uses

Application Method
Compatible Substrates & Surfaces
Typical Use Guidelines
  • This is a great ink for making electrical connections for electrochemical testing of fuel cells, ceramic substrates, electrochemical materials, and metals.
  • Stirring the ink before use is highly recommended.
  • For best results, the ink should be stirred with a spatula or a sonic wand to achieve an even consistency prior to use.
  • This ink can be used for screen printing for generating electrical connections for wire attachments.
Tips for Making Electrical Connections
  • Ensuring a solid connection between your electrodes and current collector is critical for obtaining good test results.
  • Leveraging our experience in electrochemical testing, testing we have we offer the following suggestions for obtaining optimum results with our silver paste product.

Step 1:

  • Cut or punch out the metal mesh to the size/area that you want to test on your sample.

Step 2:

  • Cut the contact wire to the desired length, with a loop around the perimeter of the mesh with the wire extending past the sample.
  • Place cut mesh in the center of your sample & the looped wire on top of wire mesh.

Step 3:

  • Apply the contact paste around the perimeter of the wire loop, apply a few drops across the mesh for best adhesion strength.

Step 4:

  • Cut and place a straight piece of wire next to the mesh on the sample.
  • Again, cover with ink for adhesion.
  • This will allow for 4 point conductivity testing and a lead for measuring voltage, while the other draws the current.

Step 5:

  • Dry in a 100°C oven for an hour or until the ink looks dry.
  • Repeat all steps on the opposite side of the sample in the same area.

Step 6:

  • Fire your sample to adhere to your contact wires.
  • Firing conditions: 1°C per minute to 800°C, hold for 1 hr, cool to room temp.sample in the same area.

Properties

Typical Properties
ValueUnitsTest Method / Conditions
Solids by Weight65 - 80%

Regulatory & Compliance

Certifications & Compliance

Packaging & Availability

Amount
  • 100g
  • 500g