Nexceris Nickel Metal Anode Ink is an excellent contact paste for SOFC testing, and is especially good for enhancing the electrical contact on the anode side of a cell during fuel cell testing. The nickel ink can also be used as a reference electrode, but any electrical testing with the nickel paste will require that the sample be under a reducing gas to maintain good electrical conductivity.

Application Area: Anode, Battery Packs, Electrical Components

Compatible Substrates & Surfaces: Ceramic, Metal

Features: Good Adhesion, Good Electrical Properties

Application Method: Screen Coating

Chemical Family: Nickel Compounds

Safety Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Chemical Family
Chemical Name
Product Type

Features & Benefits

Ready-to-Use Product Features

Applications & Uses

Application Method
Compatible Substrates & Surfaces
Typical Use Guidelines
  • This is a great ink for making electrical connections for electrochemical testing of fuel cells, ceramic substrates, electrochemical materials, and metals.
  • Stirring the ink before use is highly recommended.
  • For best results, the ink should be stirred with a spatula or a sonic wand to achieve an even consistency prior to use.
  • This ink can be used for screen printing for generating electrical connections for wire attachments.
Tips for Making Electrical Connections
  • Ensuring a solid connection between your electrodes and current collector is critical for obtaining good test results.
  • Leveraging our experience in electrochemical testing, testing we have we offer the following suggestions for obtaining optimum results with our silver paste product.

Step 1:

  • Cut or punch out the metal mesh to the size/area that you want to test on your sample.

Step 2:

  • Cut the contact wire to the desired length, with a loop around the perimeter of the mesh with the wire extending past the sample.
  • Place cut mesh in the center of your sample & the looped wire on top of wire mesh.

Step 3:

  • Apply the contact paste around the perimeter of the wire loop, apply a few drops across the mesh for best adhesion strength.

Step 4:

  • Cut and place a straight piece of wire next to the mesh on the sample.
  • Again, cover with ink for adhesion.
  • This will allow for 4 point conductivity testing and a lead for measuring voltage, while the other draws the current.

Step 5:

  • Dry in a 100°C oven for an hour or until the ink looks dry.
  • Repeat all steps on the opposite side of the sample in the same area.

Step 6:

  • Fire your sample to adhere to your contact wires.
  • Firing conditions: 1°C per minute to 800°C, hold for 1 hr, cool to room temp.sample in the same area.

Properties

Physical Form
Typical Properties
ValueUnitsTest Method / Conditions
Solids by Weight (Nickel Metal)75 - 80%-

Regulatory & Compliance

Certifications & Compliance

Packaging & Availability

Quantity

50g