Value | Units | Test Method / Conditions | |
Tensile Strength | 55 | MPa | ASTM D638 |
Tensile Modulus | 2500 | MPa | ISO 527 |
Flexural Strength | 80 | MPa | ASTM D 790 |
Flexural Modulus | 2500 | MPa | ASTM D790 |
Charpy Notched Impact Strength (-20°C) | 2 | kJ/m2 | ISO 179/1eA |
Charpy Notched Impact Strength (23°C) | 3 | kJ/m2 | ISO 179/1eA |
Charpy Impact Strength (23°C) | NB | kJ/m2 | ISO 179/1eU |
Charpy Impact Strength (-20°C) | 150 | kJ/m2 | STN EN ISO 179 |
Elongation | 8 | % | STN EN ISO 527-2 |
Value | Units | Test Method / Conditions | |
Melt Mass Flow Rate - MFR (250°C/2.1 kg) | 40 | g/10 min | STN EN ISO 1133 |
Density | 1.31 | g/cm3 | ISO 1183 |
Water Content | 0.1 | % | STN EN ISO 3344 |
Value | Units | Test Method / Conditions | |
Heat Deflection Temperature - HDT | 55 | °C | STN EN ISO 75-2 (A) |
Melting Temperature (DSC) | 200 - 220 | °C | STN EN ISO 11357-1 |
Vicat Softening Temperature (B) | 200 | °C | STN EN ISO 306 |
Value | Units | Test Method / Conditions | |
Surface Resistivity | 1.0e+15 | ohm | STN 34 6460 |
Electric Strength | 23 | kV/mm | IEC 60243-1 |
Comparative Tracking Index - CTI (A) | 600 | V | STN EN 60112 |
Volume Resistivity | 1.0e+15 | ohm.m | ASTM D 257 |
Value | Units | Test Method / Conditions | |
Glow Wire Test (3 mm) | 850 | °C | STN EN 60695-2-12 |
Flammability | HB | - | UL 94 |
Value | Units | Test Method / Conditions | |
Mold Temperature Range | 50 - 80 | °C | -- |
Drying: Temperature/Time | 120/4 | °C/h | -- |
Manufacturing Shrinkage - length/width | 1.8/1.93 | % | STN EN ISO 294-4 |
Melt Temperature Range | 250 - 270 | °C | -- |
Injection Pressure | 60 - 100 | MPa | -- |