Value | Units | Test Method / Conditions | |
Tensile Strength | 105 | MPa | ISO 527 |
Tensile Modulus | 5600 | MPa | ISO 527-2/1A/1 |
Flexural Strength | 160 | MPa | ASTM D 790 |
Flexural Modulus | 5200 | MPa | ASTM D790 |
Charpy Notched Impact Strength (23°C) | 5.5 | kJ/m2 | ISO 179/1eA |
Charpy Impact Strength (23°C) | 35 | kJ/m2 | ISO 179/1eU |
Charpy Notched Impact Strength (-20°C) | 5.5 | kJ/m2 | ISO 179 |
Charpy Impact Strength (-20°C) | 33 | kJ/m2 | ISO 179/1eU |
Elongation | 3 | % | ASTM D638 |
Value | Units | Test Method / Conditions | |
Melt Mass Flow Rate - MFR (250°C/2.16 kg) | 15 | g/10 min | STN EN ISO 1133 |
Density | 1.41 | g/cm3 | ISO 1183 |
Water Content | 0.1 | % | STN EN ISO 3344 |
Value | Units | Test Method / Conditions | |
Heat Deflection Temperature - HDT | 200 | °C | STN EN ISO 75-2 (A) |
Melting Temperature (DSC) | 200 - 220 | °C | STN EN ISO 11357-1 |
Vicat Softening Temperature (B) | 210 | °C | STN EN ISO 306 |
Value | Units | Test Method / Conditions | |
Surface Resistivity | 1.0e+15 | ohm | STN 34 6460 |
Electric Strength | 33 | kV/mm | IEC 60243-1 |
Comparative Tracking Index - CTI (A) | 350 | V | STN EN 60112 |
Volume Resistivity | 1.0e+15 | ohm.m | ASTM D 257 |
Value | Units | Test Method / Conditions | |
Glow Wire Test (3 mm) | 750 | °C | STN EN 60695-2-12 |
Flammability | HB | - | UL 94 |
Value | Units | Test Method / Conditions | |
Mold Temperature Range | 50 - 80 | °C | -- |
Drying: Temperature/Time | 120/4 | °C/h | -- |
Manufacturing Shrinkage - length/width | 0.89/1.35 | % | STN EN ISO 294-4 |
Injection Pressure | 60 - 100 | MPa | -- |
Melt Temperature Range | 250 - 280 | °C | -- |