SABIC's Specialties Business LNP THERMOCOMP EF006H compound is based on Polyetherimide (PEI) resin containing 30% glass fiber. Added features of this grade include: Healthcare. This product does not contain PFAS intentionally added during SHPP’s manufacturing process and are not expected to contain unintentional PFAS impurities. Each user is responsible for evaluating the presence of unintentional PFAS impurities.

Polymer Name: Polyether Imide (PEI)

Processing Methods: Injection Molding

Fillers Included: Glass Fiber

Flexural Modulus: 10340.0 - 10340.0 MPa

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Fillers Included
Plastics & Elastomers Functions
Technologies

Features & Benefits

Labeling Claims

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Flame Rating
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Stress (Break) ¹¹166MPaASTM D638
Tensile Strain (Break) ¹¹2.3%ASTM D638
Tensile Modulus (at 50 mm/min) ¹¹10340MPaASTM D638
Flexural Stress ¹¹262MPaASTM D790
Flexural Modulus ¹¹10340MPaASTM D790
Physical Properties
ValueUnitsTest Method / Conditions
Density ¹¹1.52g/cm³ASTM D792
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature (at 1.82 MPa, 3.2mm, Unannealed) ¹¹204°CASTM D648
Relative Temperature Index (Electrical) ᵖ ¹¹105°CUL 746B
Relative Temperature Index (Mechanical with impact) ᵖ ¹¹105°CUL 746B
Relative Temperature Index (Mechanical without impact) ᵖ ¹¹105°CUL 746B
Impact Properties
ValueUnitsTest Method / Conditions
Izod Impact (Unnotched, at 23°C) ¹¹640J/mASTM D4812
Izod Impact (Notched, at 23°C) ¹¹85J/mASTM D256
Injection Molding
ValueUnitsTest Method / Conditions
Drying Temperature ⁷150°C
Drying Time ⁷4 - 6Hrs
Maximum Moisture Content ⁷0.02%
Melt Temperature ⁷360 - 400°C
Rear - Zone 1 Temperature ⁷360 - 380°C
Middle - Zone 2 Temperature ⁷370 - 390°C
Front - Zone 3 Temperature ⁷380 - 400°C
Nozzle Temperature ⁷390 - 400°C
Mold Temperature ⁷140 - 180°C
Back Pressure ⁷0.3 - 0.7MPa
Screw Speed (Circumferential speed) ⁷0.2 - 0.3m/s
Vent Depth ⁷0.025 - 0.076mm
Flame Characteristics
ValueUnitsTest Method / Conditions
UL Recognized (94V-0 Flame Class Rating) ᵖmin. 0.75mmUL 94
Note
  • ᵖ UL ratings shown on the technical datasheet might not cover the full range of thicknesses and colors. For details, please see the UL Yellow Card.
  • ⁷ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding.
  • ¹¹ The information stated on Technical Datasheets should be used as indicative only for material selection purposes and not be utilized as specification or used for part or tool design.
 

Regulatory & Compliance

Certifications & Compliance

Packaging & Availability

Regional Availability
  • Americas
  • Asia
  • Europe
  • North America