Knowde Enhanced TDS
Identification & Functionality
- Product Type
- Technologies
- Product Families
Features & Benefits
- Ready-to-Use Product Features
Applications & Uses
- Applications
- Application Method
- Compatible Substrates & Surfaces
- Hardened Glass Surface Preparation
-
- Plasma cleaning: If the hardened glass is hydrophilic, plasma treatment is not required. If the glass is hydrophobic (water contact angle >5°) argon plasma treatment for 5 minutes is recommended.
- Acid treatment: Immerse the hardened glass in 5% hydrochloric acid (HCL) for 4 hours. Rinse the glass with deionized water.
- Water soak: Submerge the glass in deionized water for 18 hours and dry by heating at 90°C.
- Apply 3750Y: Dip the cleaned hardened glass for 1 min in FluoroSyl 3750Y at 0.2% and then bake the glass at 150°C for 1.5 hours with 50% relative humidity. Vapor deposition and spraying can also be used to apply FluoroSyl 3750Y