- The high melting point of VESTAMID Terra DS16 compounds results in a high heat deflection temperature that can be advantageous for some applications.
- VESTAMID® Terra DS16 occupies a position between the high-performance long-chain polyamides such as PA 12 and PA 1212 and the standard polyamides PA 6 and PA 66, which have a shorter chain length.
- VESTAMID® Terra is a group of new polyamides, the monomers for which are based entirely or partly on renewable raw materials.
- VESTAMID® Terra DS is the polycondensation product of 1,10-decamethylene diamine (D) and 1,10-dodecanedioic acid (sebacic acid-S). Because both monomers are extracted from castor oil, VESTAMID® Terra DS is based on natural, bio-based and renewable resources up to 100%.
Applications & Uses
- Plastics & Elastomers End Uses
- Plastics & Elastomers Processing Methods
Properties
- Flame Rating
- Mechanical Properties
- Thermal Properties
- Electrical Properties
- Other Properties
- Rheological Properties
Value | Units | Test Method / Conditions | |
Tensile Modulus (dry) | 1700 | MPa | ISO 527-1/-2 |
Tensile Modulus (cond.) | 1250 | MPa | ISO 527-1/-2 |
Yield Stress (dry) | 54 | MPa | ISO 527-1/-2 |
Yield Stress (cond.) | 48 | MPa | ISO 527-1/-2 |
Yield Strain (dry) | 5 | % | ISO 527-1/-2 |
Yield Strain (cond.) | 22 | % | ISO 527-1/-2 |
Nominal Strain at Break (dry) | min. 50 | % | ISO 527-1/-2 |
Nominal Strain at Break (cond.) | min. 50 | % | ISO 527-1/-2 |
Charpy Notched Impact Strength (+23°C, dry) | 7C | kJ/m² | ISO 179/1eA |
Charpy Notched Impact Strength (+23°C, cond.) | 7C | kJ/m² | ISO 179/1eA |
Charpy Notched Impact Strength (-30°C, dry) | 7C | kJ/m² | ISO 179/1eA |
Charpy Notched Impact Strength (-30°C, cond.) | 5C | kJ/m² | ISO 179/1eA |
Value | Units | Test Method / Conditions | |
Melting Temperature (10°C/min, dry) | 200 | °C | ISO 11357-1/-3 |
Glass Transition Temperature (10°C/min, dry) | 37 | °C | 1SO 11357-1/-2 |
Temperature of Deflection Under Load (1.80 Mpa, dry) | 55 | °C | 150 75-1/-2 |
Temperature of Deflection Under Load (0.45 Mpa, dry) | 136 | °C | 150 75-1/-2 |
Vicat Softening Temperature (50°C/h 50N, dry) | 171 | °C | ISO 306 |
Coefficient of Linear Thermal Expansion (Parallel, dry) | 115 | E-6/K | ISO 11359-1/-2 |
Coefficient of Linear Thermal Expansion (Normal, dry) | 135 | E-6/K | ISO 11359-1/-2 |
Burning Behavior (at 1.5 mm Nominal Thickness) (dry) | HB | class | IEC 60695-11-10 |
Value | Units | Test Method / Conditions | |
Relative Permittivity (100Hz, dry) | 3.6 | — | IEC 62631-2-1 |
Relative Permittivity (1MHz, dry) | 31 | — | IEC 62631-2-1 |
Volume Resistivity (dry) | min. 1E13 | Ohm*m | IEC 62631-3-1 |
Volume Resistivity (cond.) | 830000000000 | Ohm*m | IEC 62631-3-1 |
Electric Strength (dry) | 37 | kv/mm | IEC 60243-1 |
Value | Units | Test Method / Conditions | |
Water Absorption (dry) | 1.8 | % | Sim. to ISO 62 |
Humidity Absorption (dry) | 1.4 | % | Sim. to ISO 62 |
Density (dry) | 1040 | kg/m³ | 1SO 1183 |
Value | Units | Test Method / Conditions | |
Molding Shrinkage (Parallel, dry) | 1.4 | % | ISO 294-4, 2577 |
Molding Shrinkage (Normal, dry) | 1.5 | % | ISO 294-4, 2577 |
Packaging & Availability
- Regional Availability
- Packaging Information
VESTAMID® Terra DS16 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags.