LNP™ STAT-LOY™ Compound A3000TXB

1 of 27 products in this brand
SABIC's Specialties Business LNP STAT-LOY A3000TXB compound is based on Acrylonitrile Butadiene Styrene (ABS) resin containing proprietary fillers. Added features of this grade include: Permanently Anti-Static, Transparent, Bio-assessed to ISO 10993. This product does not contain PFAS intentionally added during SHPP’s manufacturing process and are not expected to contain unintentional PFAS impurities. Each user is responsible for evaluating the presence of unintentional PFAS impurities.

Polymer Name: Acrylonitrile Butadiene Styrene (ABS)

Fillers Included: Proprietary

Processing Methods: Injection Molding

Additives Included: Anti-Static Agent, UV Stabilizer

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Fillers Included
Plastics & Elastomers Functions
Technologies

Features & Benefits

Product Features
  • Dimensional stability, transparency and biocomp assessed (ISO10993 certified)

Applications & Uses

Plastics & Elastomers Processing Methods
Product Applications
  • Inhalers
  • Pill sorter covers

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Stress (Yield, Type I, 5 mm/min) ¹¹38MPaASTM D638
Tensile Stress (Break, Type I, 5 mm/min) ¹¹27MPaASTM D638
Tensile Strain (Yield, Type I, 5 mm/min) ¹¹4%ASTM D638
Tensile Strain (Break, Type I, 5 mm/min) ¹¹31%ASTM D638
Tensile Modulus (at 5 mm/min) ¹¹1660MPaASTM D638
Flexural Stress (Yield, 1.3 mm/min, 50 mm span) ¹¹54MPaASTM D790
Flexural Modulus (at 1.3 mm/min, 50 mm span) ¹¹1630MPaASTM D790
Tensile Stress (Yield, 5 mm/min) ¹¹37MPaISO 527
Tensile Stress (Break, 5 mm/min) ¹¹26MPaISO 527
Tensile Strain (Yield, 5 mm/min) ¹¹4%ISO 527
Tensile Strain (Break, 5 mm/min) ¹¹29%ISO 527
Tensile Modulus (at 1 mm/min) ¹¹1550MPaISO 527
Flexural Stress ¹¹49MPaISO 178
Flexural Modulus (at 2 mm/min) ¹¹1490MPaISO 178
Physical Properties
ValueUnitsTest Method / Conditions
Specific Gravity ¹¹1.09ASTM D792
Density ¹¹1.08g/cm³ASTM D792
Moisture Absorption (at 23°C, 50% RH, 24hrs) ¹¹0.54%ASTM D570
Mold Shrinkage (flow, 24 hrs) ᵍ ¹¹0.4 - 0.6%ASTM D955
Mold Shrinkage (xflow, 24 hrs) ᵍ ¹¹0.6 - 0.8%ASTM D955
Moisture Absorption (at 23°C, 50% RH) ¹¹0.81%ISO 62
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature (at 0.45 MPa, 3.2 mm, Unannealed) ¹¹78°CASTM D648
Heat Deflection Temperature (at 1.82 MPa, 3.2mm, Unannealed) ¹¹66°CASTM D648
Coefficient of Thermal Expansion (at -30°C to 30°C, flow) ¹¹0.000011/°CASTM D696
Coefficient of Thermal Expansion (at -30°C to 30°C, xflow) ¹¹0.0001091/°CASTM D696
Heat Deflection Temperature/Bf (at 0.45 Mpa, Flatw 80*10*4, sp=64mm) ¹¹77°CISO 75/Bf
Heat Deflection Temperature/Af (at 1.8 Mpa, Flatw 80*10*4, sp=64mm) ¹¹66°CISO 75/Af
Electrical Properties
ValueUnitsTest Method / Conditions
Volume Resistivity ᵈ ¹¹10000000000 - 1000000000000Ω.cmASTM D257
Surface Resistivity ᵈ ¹¹1000000000 - 100000000000ΩASTM D257
Static Decay (at 5000V to max. 50V) ¹¹max. 1SecondsFTMS101B
Impact Properties
ValueUnitsTest Method / Conditions
Izod Impact (Notched, at 23°C) ¹¹131J/mASTM D256
Multi-Axial Impact ¹¹33JISO 6603
Instrumented Dart Impact Total Energy (at 23°C) ¹¹20JASTM D3763
Izod Impact (Notched, 80*10*4, at 23°C) ¹¹14kJ/m²ISO 180/1A
Injection Molding
ValueUnitsTest Method / Conditions
Drying Temperature ⁷70 - 80°C
Drying Time ⁷4Hrs
Maximum Moisture Content ⁷0.05 - 0.1%
Melt Temperature ⁷200 - 210°C
Front - Zone 3 Temperature ⁷205 - 215°C
Middle - Zone 2 Temperature ⁷195 - 205°C
Rear - Zone 1 Temperature ⁷180 - 195°C
Mold Temperature ⁷10 - 50°C
Back Pressure ⁷0.2 - 0.3MPa
Screw Speed ⁷30 - 60rpm
Note
  • ᵈ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding. Do NOT mix NORYL GTX* resin with other grades of NORYL* resins. Polystyrene and acrylic regrind are effective purging Materials. Use temperature range appropriate for particular purging resin. Regrind must also be dried. Maximum 25% regrind. Dry at recommended temperatures and times for optimum performance. Overdrying can cause loss of physical properties and/or create appearance defects. Do not exceed recommended basic drying time and temperature above or:\n4-8 hrs at 95°C (200°F), 10 hrs max\n6-12 hrs at 80°C (175°F), 16 hrs max\n8-16 hrs at 65°C (150°F), 24 hrs max\nAVOID air circulating tray ovens. Moisture levels in heated ambient air can exceed moisture level in the resin itself, causing moisture ABSORPTION not drying. Avoid melt temperature in excess of 300°C (575°F) and residence times over 6-8 minutes (may affect properties and/or appearance). Nozzle temperature controls assist in elimination of drool premature freeze-off. Shot sizes in excess of 50% barrel capacity can lead to difficulties in providing a consistent, homogenous plastic melt.
  • ᵍ Measurements made from Laboratory test Coupon. Actual shrinkage may vary outside of range due to differences in processing conditions, equipment, part geometry and tool design. It is recommended that mold shrinkage studies be performed with surrogate or legacy tooling prior to cutting tools for new molded article.
  • ⁷ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding.
  • ¹¹ The information stated on Technical Datasheets should be used as indicative only for material selection purposes and not be utilized as specification or used for part or tool design.
 