SABIC's Specialties Business NORYL GTX870 resin is a 20% glass reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits high stiffness, excellent chemical resistance, and high heat resistance. NORYL GTX870 resin is an excellent candidate for a wide variety of applications including electrical connectors and electronic base stations. This product does not contain PFAS intentionally added during SHPP’s manufacturing process and are not expected to contain unintentional PFAS impurities. Each user is responsible for evaluating the presence of unintentional PFAS impurities.

Polymer Name: PPO/Nylon Alloy

Processing Methods: Injection Molding

Density: 1240.0 - 1240.0 kg/m³

Flexural Modulus: 5680.0 - 5680.0 MPa

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Fillers Included
Polymer Name
Plastics & Elastomers Functions
Technologies

Features & Benefits

Labeling Claims

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Stress (Yield)117MPaSABIC - Japan Method
Tensile Stress (Yield, Type I, 5 mm/min)122MPaASTM D638
Tensile Strain (Break)12%SABIC - Japan Method
Tensile Strain (Break, Type I, 5 mm/min)5%ASTM D638
Flexural Modulus5680MPaASTM D790
Flexural Stress166MPaASTM D790
Physical Properties
ValueUnitsTest Method / Conditions
Water Absorption (at 23°C, 24hrs)0.5%ASTM D570
Mold Shrinkage (flow, 3.2 mm)0.4 - 0.8%SABIC method
Specific Gravity1.24ASTM D792
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature (at 1.82 MPa, 6.4 mm, Unannealed)200°CASTM D648
Coefficient of Thermal Expansion (at -30°C to 30°C)0.00004 - 0.000061/°CTMA
Impact Properties
ValueUnitsTest Method / Conditions
Izod Impact (Notched, at 23°C)117J/mASTM D256
Injection Molding
ValueUnitsTest Method / Conditions
Back Pressure0.3 - 1.4MPa
Drying Temperature95 - 105°C
Drying Time3 - 4Hrs
Drying Time (Cumulative)8Hrs
Front - Zone 3 Temperature275 - 305°C
Maximum Moisture Content0.07%
Melt Temperature280 - 305°C
Middle - Zone 2 Temperature270 - 305°C
Mold Temperature75 - 120°C
Nozzle Temperature280 - 305°C
Rear - Zone 1 Temperature265 - 305°C
Screw Speed20 - 100rpm
Shot to Cylinder Size30 - 50%
Vent Depth0.013 - 0.038mm