Tear Strength: 30.0 - 30.0 kN/m

Strain at Break: 540.0 - 540.0 %

    Knowde Enhanced TDS

    Identification & Functionality

    Chemical Family
    Technologies

    Applications & Uses

    Plastics & Elastomers Processing Methods

    Properties

    Mechanical Properties
    ValueUnitsTest Method / Conditions
    Tensile Strength4.8MPaASTM D 638
    Hardness70Shore AISO 7619-1
    Strain at break540%ISO 37
    Tear Strength30kN/mASTM D624
    Physical Properties
    ValueUnitsTest Method / Conditions
    Melt Flow Index - MFI (190°C/5 kg)30g/10 minASTM D 1238
    Density1000kg/m3ISO 1183