Polymer Name: Styrenic Thermoplastic Elastomer

Processing Methods: Injection Molding

Tear Strength: 17.0 - 17.0 kN/m

Strain at Break: 660.0 - 660.0 %

Compression Set (70 °C): 60.0 - 60.0 %

    Knowde Enhanced TDS

    Identification & Functionality

    Chemical Family
    Technologies

    Applications & Uses

    Plastics & Elastomers Processing Methods

    Properties

    Mechanical Properties
    ValueUnitsTest Method / Conditions
    Tensile Strength3.2MPaISO 37
    Hardness40Shore AISO 7619-1
    Strain at break660%ISO 37
    Compression set (70°, 24h)60%ISO 815
    Compression set (23°, 24h)14%ISO 815
    Compression set (100°, 24h)83%ISO 815
    Tear Strength17kN/mASTM D 624
    Physical Properties
    ValueUnitsTest Method / Conditions
    Melt Flow Index - MFI (190°C/5 kg)20g/10 minASTM D 1238
    Density1060kg/m3ISO 1183

    Packaging & Availability