Polymer Name: Styrenic Thermoplastic Elastomer

Processing Methods: Injection Molding

Tear Strength: 15.0 - 15.0 kN/m

Strain at Break: 700.0 - 700.0 %

Compression Set (70 °C): 60.0 - 60.0 %

    Knowde Enhanced TDS

    Identification & Functionality

    Chemical Family
    Technologies

    Applications & Uses

    Plastics & Elastomers Processing Methods

    Properties

    Mechanical Properties
    ValueUnitsTest Method / Conditions
    Tensile Strength3MPaISO 527
    Hardness40Shore AISO 7619-1
    Strain at break700%ISO 37
    Compression set (70°, 24h)60%ISO 815
    Compression set (23°, 24h)13%ISO 815
    Compression set (100°, 24h)82%ISO 815
    Tear Strength15kN/mISO 34-1
    Physical Properties
    ValueUnitsTest Method / Conditions
    Melt Flow Index - MFI (190°C/5 kg)9g/10 minASTM D 1238
    Density1150kg/m3ISO 1183

    Packaging & Availability

    Regional Availability