Polymer Name: Styrenic Thermoplastic Elastomer

Processing Methods: Injection Molding

Tear Strength: 58.0 - 58.0 kN/m

Strain at Break: 520.0 - 520.0 %

Compression Set (70 °C): 90.0 - 90.0 %

    Knowde Enhanced TDS

    Identification & Functionality

    Chemical Family
    Technologies

    Applications & Uses

    Plastics & Elastomers Processing Methods

    Properties

    Mechanical Properties
    ValueUnitsTest Method / Conditions
    Tensile Strength10.3MPaASTM D 638
    Hardness40Shore DISO 7619-1
    Strain at break520%ISO 37
    Compression set (23°, 24h)36%ISO 815
    Compression set (70°, 24h)90%ISO 815
    Tear Strength58kN/mASTM D 624
    Physical Properties
    ValueUnitsTest Method / Conditions
    Melt Flow Index - MFI (190°C/5 kg)13.6g/10 minISO 1133
    Density1110kg/m3ISO 1183

    Packaging & Availability

    Regional Availability