Solplast™ TH 45A8003 A

1 of 994 products in this brand

Polymer Name: Styrenic Thermoplastic Elastomer

Processing Methods: Injection Molding

Tear Strength: 18.0 - 18.0 kN/m

Strain at Break: 640.0 - 640.0 %

Compression Set (70 °C): 61.0 - 61.0 %

    Knowde Enhanced TDS

    Identification & Functionality

    Chemical Family
    Technologies

    Applications & Uses

    Plastics & Elastomers Processing Methods

    Properties

    Mechanical Properties
    ValueUnitsTest Method / Conditions
    Tensile Strength3.8MPaASTM D 638
    Hardness45Shore AASTM D 2240
    Strain at break640%ISO 37
    Compression set (70°, 24h)61%ISO 815
    Compression set (23°, 24h)14%ISO 815
    Compression set (100°, 24h)83%ISO 815
    Tear Strength18kN/mISO 34-1
    Physical Properties
    ValueUnitsTest Method / Conditions
    Melt Flow Index - MFI (190°C/5 kg)14g/10 minASTM D 1238
    Density1060kg/m3ISO 1183