Polymer Name: Styrenic Thermoplastic Elastomer

Processing Methods: Injection Molding

Tear Strength: 15.0 - 15.0 kN/m

Strain at Break: 870.0 - 870.0 %

Compression Set (70 °C): 26.0 - 26.0 %

    Knowde Enhanced TDS

    Identification & Functionality

    Chemical Family
    Technologies

    Applications & Uses

    Plastics & Elastomers Processing Methods

    Properties

    Mechanical Properties
    ValueUnitsTest Method / Conditions
    Tensile Strength6.8MPaISO 37
    Hardness45Shore AASTM D 2240
    Strain at break870%ISO 37
    Compression set (100°, 24h)45%ISO 815
    Compression set (70°, 24h)26%ISO 815
    Compression set (23°, 24h)14%ISO 815
    Tear Strength15kN/mISO 34-1
    Physical Properties
    ValueUnitsTest Method / Conditions
    Melt Flow Index - MFI (190°C/5 kg)7.8g/10 minISO 1133
    Density900kg/m3ASTM D 792

    Packaging & Availability

    Regional Availability
    • Europe