Uteksol Company Logo

Solplast™ TH 50A7000 A0

1 of 994 products in this brand

Polymer Name: Styrenic Thermoplastic Elastomer

Processing Methods: Injection Molding

Tear Strength: 22.0 - 22.0 kN/m

Strain at Break: 550.0 - 550.0 %

Compression Set (70 °C): 90.0 - 90.0 %

    Knowde Enhanced TDS

    Identification & Functionality

    Chemical Family
    Technologies

    Applications & Uses

    Plastics & Elastomers Processing Methods

    Properties

    Color
    Mechanical Properties
    ValueUnitsTest Method / Conditions
    Tensile Strength4MPaASTM D 638
    Hardness50Shore AASTM D 2240
    Strain at break550%ISO 37
    Compression set (23°, 24h)15%ISO 815
    Compression set (70°, 24h)90%ISO 815
    Tear Strength22kN/mISO 34-1
    Physical Properties
    ValueUnitsTest Method / Conditions
    Melt Flow Index - MFI (190°C/5 kg)23g/10 minISO 1133
    Density970kg/m3ISO 1183

    Packaging & Availability

    Regional Availability
    • Europe