VESTAMID® X7393 NC is a high-viscosity, plasticized, impact-modified, heat- and light-stabilized polyamide 12 compound used for flexible tubing and hoses in the automobile industry. Parts made from VESTAMID® X7393 NC exhibit optimized cold temperature impact resistance and increased burst pressure resistance in the extrusion of semi-rigid tubing. Additionally, it offers an exceptional low coefficient of friction and good chemical resistance.

Polymer Name: Polyamide 12 (PA 12)

Processing Methods: Extrusion, Injection Molding

Additives Included: Heat Stabilizer, Impact Modifier, Light Stabilizer, Plasticizer (Unspecified)

Flexural Modulus: 499.525 - 499.525 MPa

Materials Features: Chemical Resistant, Electrically Insulating, Flexible, Fuel Resistant, Good Light Stability, Good Thermal Stability, Good Weather Stability, Heat Stabilized, High Pressure Resistance, High Viscosity, Impact Modified, Impact Resistance, Light Stabilized, Low Coefficient of Friction, Low Moisture Absorption, Low Temperature Impact Resistance, Oil Resistant, Plasticized, Semi Rigid, UV Resistant, Unreinforced

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Chemical Family
Plastics & Elastomers Functions
Technologies

Features & Benefits

Product Attributes

Parts made of VESTAMID® X7393 are characterized by optimized cold temperature impact resistance for the extrusion of semi-rigid tubing with increased burst pressure resistance as well as exceptional low coefficient of friction and good chemical resistance. Properties of compounds based on Polyamide 12 vary little with changing humidity due to their low moisture absorption.

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Physical Form
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Modulus (dry)75400psiISO 527
Tensile Modulus (cond.)68200psiISO 527
Tensile Strength (dry)4210psiISO 527
Tensile Strength (cond.)3920psiISO 527
Yield Stress (dry)4210psiISO 527
Yield Stress (cond.)3920psiISO 527
Yield Strain (dry)28%ISO 527
Yield Strain (cond.)28%ISO 527
Stress at 50% Strain (dry)4210psiISO 527
Stress at 50% Strain (cond.)3770psiISO 527
Stress at Break (dry)6090psiISO 527
Stress at Break (cond.)6090psiISO 527
Nominal Strain at Break (ɛtb, dry)200%ISO 527
Nominal Strain at Break (ɛtb, cond.)210%ISO 527
Charpy Notched Impact Strength (+23°C, dry)51.4ftlb/in²ISO 179/1eA
Charpy Notched Impact Strength (+23°C, cond.)61.8ftlb/in²ISO 179/1eA
Charpy Notched Impact Strength (-30°C, dry)3.33ftlb/in²ISO 179/1eA
Charpy Notched Impact Strength (-30°C, cond.)3.81ftlb/in²ISO 179/1eA
Flexural Modulus (23°C, dry)72500psiISO 178
Flexural Modulus (23°C, cond.)65300psiISO 178
Flexural Stress at Conv. Deflection (23°C, dry)2470psiISO 178
Flexural Stress at Conv. Deflection (23°C, cond.)2320psiISO 178
Flexural Strength (23°C, dry)3630psiISO 178
Flexural Strength (23°C, cond.)3630psiISO 178
Flexural Strain at Flexural Strength (23°C, dry)9%ISO 178
Flexural Strain at Flexural Strength (23°C, cond.)10%ISO 178
Physical Properties
ValueUnitsTest Method / Conditions
Density (dry)1.02g/cm³ISO 1183
Water Absorption (dry)1.2%Sim. to 1SO 62
Humidity Absorption (dry)0.7%Sim. to 1SO 62
Moisture Content (dry)0.03wt.-%ISO 15512
Bulk Density (Granulate)37.2Ib/ft³
Weight Per 1000 Granules (dry)14.9g
Shore D Hardness (dry)67ISO 7619-1
Thermal Properties
ValueUnitsTest Method / Conditions
Melting Temperature (dry)351°F
Glass Transition Temperature (dry)59°F
Temperature of Deflection Under Load A (1.80 Mpa, dry)113°F
Temperature of Deflection Under Load B (0.45 Mpa, dry)230°F
Vicat Softening Temperature A (10 N, 50 K/h, dry)338°F
Vicat Softening Temperature B (50 N, 50 K/h, dry)257°F
Optical Properties
ValueUnitsTest Method / Conditions
Color b4.29CIE
Test Specimen Production
ValueUnitsTest Method / Conditions
Injection Molding - Melt Temperature 428°FISO 294
Injection Molding - Mold Temperature 140°FISO 294
Injection Molding - Injection Velocity 7.87in/sISO 294
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Volume Flow Rate (dry, at 446°F, 11lb)8.5cm³/10minISO 1133
Molding Shrinkage (Parallel, dry)0.8%ISO 294-4, 2577
Molding Shrinkage (Normal, dry)14%ISO 294-4, 2577

Regulatory & Compliance

Quality Standards

Packaging & Availability

Packaging Information

VESTAMID® X7393 is supplied as pellets, ready for use, in moisture-proof bags.

Storage & Handling

Shelf Life
2 years
Storage Conditions

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.