UNI-REZ 2651 hot melt polyamide adhesive is a resin based on dimer acid. UNI-REZ 2651 hot melt polyamide adhesive has excellent low temperature impact resistance and good adhesion to polyolefin.

Chemical Family: Polyamides

End Uses: Hot Melt Adhesive

Features: Excellent Adhesion, Water Resistance

Similar Products

  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Chemical Family
CASE Ingredients Functions
Technologies

Features & Benefits

CASE Ingredients Features
Product Highlights
  • Low heat reactivation
  • Low temperature flexibility
  • Water resistance

Applications & Uses

Adhesive & Sealant Type
Applications
  • Heat shrink sleeves
  • Automotive wire splice

Properties

Sales Specifications
ValueUnitsTest Method / Conditions
Softening Point (Ring & Ball)95 - 105°CASTM E28 (AQCM 003)
Viscosity LVT Brookfield, Spindle #31, cps/mPA.s 190°C5000 - 7000ASTM D3236 (AQCM 146)
Color , 40% in n-Butanolmax. 7GardnerAQCM 002
Typical Properties
ValueUnitsTest Method / Conditions
Acid Number0.9mg KOH/gAQCM 001
Amine Number4.5mg KOH/gAQCM 139
Moisture Quintel Moisture Analyzer0.19%AQCM 056
Color , 40% in n-Butanol5.0GardnerAQCM 002
Tensile Strength380 (2.6)MpaASTM D1708
Elongation at Break550.0%ASTM D1708
Tensile Modulus9500 (65)MpaASTM D638
Mandrel Bend Flexibility (1” diameter), pass-30.0°CASTM D3111
Open Time seconds, 10 mil film5.0ASTM D4497
Shear Adhesion Failure Temp (SAFT), 1 kg. wt. C85.0ASTM D4498
Hardness86Shore AASTM D2240-97
Pounds per gallon 25°C8.0 (0.96)g/ccASTM D792
Flash Point (COC)271 (520)°C (°F)ASTM D92-16

Technical Details & Test Data

Viscosity/Temperature Curve

Kraton UNI-REZ 2651 Viscosity/Temperature Curve

Packaging & Availability

Packaging
  • UNI-REZ 2651 hot melt polyamide adhesive is in pellet form, packaged in poly-foil lined multi-wall bags, 40 or 50 lb . net

Storage & Handling

Storage

This product will slowly absorb moisture from the air, which may cause foaming when the resin is melted and could result in inadequate bonds. Partially used containers should be closed tightly, or the remaining resin transferred into an airtight container and kept in a cool, dry area.