SABIC's Specialties Business LNP THERMOCOMP MF002S compound is based on Polypropylene (PP) resin containing 10% glass fiber. Added features of this grade include: Heat Stabilized. This product does not contain PFAS intentionally added during SHPP’s manufacturing process and are not expected to contain unintentional PFAS impurities. Each user is responsible for evaluating the presence of unintentional PFAS impurities.

Polymer Name: Polypropylene (unspecified)

Processing Methods: Injection Molding

Additives Included: Heat Stabilizer

Fillers Included: Glass Fiber

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Fillers Included
Plastics & Elastomers Functions
Technologies

Features & Benefits

Labeling Claims

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Flame Rating
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Stress (Yield, 5 mm/min) ¹¹53MPaISO 527
Tensile Stress (Yield, 5 mm/min) ¹¹46MPaISO 527
Tensile Stress (Break, 5 mm/min) ¹¹44MPaISO 527
Tensile Stress (Break, 5 mm/min) ¹¹51MPaISO 527
Tensile Stress (Yield, Type I, 5 mm/min) ¹¹46MPaASTM D638
Tensile Strain (Yield, 5 mm/min) ¹¹4%ISO 527
Tensile Strain (Yield, 5 mm/min) ¹¹4.4%ISO 527
Tensile Stress (Break, Type I, 5 mm/min) ¹¹42MPaASTM D638
Tensile Strain (Break, 5 mm/min) ¹¹4.1%ISO 527
Tensile Strain (Break, 5 mm/min) ¹¹5.8%ISO 527
Tensile Modulus (at 1 mm/min) ¹¹2970MPaISO 527
Tensile Strain (Yield, Type I, 5 mm/min) ¹¹4.7%ASTM D638
Flexural Stress (Yield, at 2 mm/min) ¹¹74MPaISO 178
Tensile Strain (Break, Type I, 5 mm/min) ¹¹6.7%ASTM D638
Flexural Modulus (at 2 mm/min) ¹¹2330MPaISO 178
Tensile Modulus (at 50 mm/min) ¹¹2980MPaASTM D638
Flexural Stress ¹¹75MPaASTM D790
Flexural Stress ¹¹64MPaISO 178
Flexural Modulus (at 1.3 mm/min, 50 mm span) ¹¹2390MPaASTM D790
Physical Properties
ValueUnitsTest Method / Conditions
Mold Shrinkage (flow) ᵍ ¹¹0.3 - 0.7%SABIC method
Density ¹¹0.97g/cm³ISO 1183
Density ¹¹0.96g/cm³ASTM D792
Water Absorption (at 23°C, 24hrs) ¹¹0.01%ISO 62-1
Specific Gravity ¹¹0.97ASTM D792
Mold Shrinkage (flow, 24 hrs) ᵍ ¹¹1 - 3%ASTM D955
Mold Shrinkage (xflow, 24 hrs) ᵍ ¹¹1 - 3%ASTM D955
Moisture Absorption (at 23°C, 50% RH) ¹¹0.01%ISO 62
Thermal Properties
ValueUnitsTest Method / Conditions
Coefficient of Thermal Expansion (at 23°C to 60°C, flow) ¹¹0.0000681/°CISO 11359-2
Heat Deflection Temperature/Bf (at 0.45 Mpa, Flatw 80*10*4, sp=64mm) ¹¹146°CISO 75/Bf
Heat Deflection Temperature/Af (at 1.8 Mpa, Flatw 80*10*4, sp=64mm) ¹¹106°CISO 75/Af
Heat Deflection Temperature/Af (at 1.8 Mpa, Flatw 80*10*4, sp=64mm) ¹¹99°CISO 75/Af
Relative Temperature Index (Electrical) ᵖ ¹¹65°CUL 746B
Relative Temperature Index (Mechanical with impact) ᵖ ¹¹65°CUL 746B
Relative Temperature Index (Mechanical without impact) ᵖ ¹¹65°CUL 746B
Heat Deflection Temperature (at 0.45 MPa, 3.2 mm, Unannealed) ¹¹154°CASTM D648
Heat Deflection Temperature (at 1.82 MPa, 3.2mm, Unannealed) ¹¹113°CASTM D648
Coefficient of Thermal Expansion (at -30°C to 30°C, flow) ¹¹0.0000661/°CASTM D696
Coefficient of Thermal Expansion (at -30°C to 30°C, xflow) ¹¹0.0000881/°CASTM D696
Electrical Properties
ValueUnitsTest Method / Conditions
Comparative Tracking Index (UL, PLC) ¹¹0PLC CodeUL 746A
Hot Wire Ignition (PLC 2) ¹¹min. 3mmUL 746A
Hot Wire Ignition (PLC 3) ¹¹min. 1mmUL 746A
High Ampere Arc Ignition (PLC 1) ¹¹min. 1.5mmUL 746A
High Ampere Arc Ignition (PLC 3) ¹¹min. 1mmUL 746A
High Voltage Arc Track Rate (PLC) ¹¹1PLC CodeUL 746A
Arc Resistance (Tungsten, PLC) ¹¹6PLC CodeASTM D495
Impact Properties
ValueUnitsTest Method / Conditions
Izod Impact (Unnotched, 80*10*4, at 23°C) ¹¹35kJ/m²ISO 180/1U
Izod Impact (Unnotched, 80*10*4, at 23°C) ¹¹29kJ/m²ISO 180/1U
Izod Impact (Notched, 80*10*4, at 23°C) ¹¹8kJ/m²ISO 180/1A
Izod Impact (Notched, 80*10*4, at 23°C) ¹¹5kJ/m²ISO 180/1A
Izod Impact (Unnotched, at 23°C) ¹¹488J/mASTM D4812
Izod Impact (Notched, at 23°C) ¹¹38J/mASTM D256
Multi-Axial Impact ¹¹1JISO 6603
Instrumented Dart Impact Total Energy (at 23°C) ¹¹4JASTM D3763
Injection Molding
ValueUnitsTest Method / Conditions
Drying Temperature ⁷80°C
Drying Time ⁷4Hrs
Melt Temperature ⁷225 - 250°C
Front - Zone 3 Temperature ⁷240 - 250°C
Middle - Zone 2 Temperature ⁷215 - 225°C
Rear - Zone 1 Temperature ⁷195 - 205°C
Mold Temperature ⁷30 - 50°C
Back Pressure ⁷0.2 - 0.3MPa
Screw Speed ⁷30 - 60rpm
Flame Characteristics
ValueUnitsTest Method / Conditions
UL Recognized (94HB Flame Class Rating) ᵖmin. 1mmUL 94
Glow Wire Ignitability Temperature (at 3.0 mm) ᵖ875°CIEC 60695-2-13
Glow Wire Ignitability Temperature (at 1.5 mm) ᵖ850°CIEC 60695-2-13
Glow Wire Flammability Index (at 3 mm) ᵖ850°CIEC 60695-2-12
Glow Wire Flammability Index (at 1.5 mm) ᵖ850°CIEC 60695-2-12
Note
  • ᵍ Measurements made from Laboratory test Coupon. Actual shrinkage may vary outside of range due to differences in processing conditions, equipment, part geometry and tool design. It is recommended that mold shrinkage studies be performed with surrogate or legacy tooling prior to cutting tools for new molded article.
  • ᵖ UL ratings shown on the technical datasheet might not cover the full range of thicknesses and colors. For details, please see the UL Yellow Card.
  • ⁷ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding.
  • ¹¹ The information stated on Technical Datasheets should be used as indicative only for material selection purposes and not be utilized as specification or used for part or tool design.
 