LNP™ THERMOCOMP™ Compound NF004

1 of 486 products in this brand
SABIC's Specialties Business LNP THERMOCOMP NF004 compound is based on Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend containing 20% glass fiber. This product does not contain PFAS intentionally added during SHPP’s manufacturing process and are not expected to contain unintentional PFAS impurities. Each user is responsible for evaluating the presence of unintentional PFAS impurities.

Polymer Name: PC/ABS Alloy

Processing Methods: Injection Molding

Density: 1300.0 - 1300.0 kg/m³

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Fillers Included
Polymer Name
Plastics & Elastomers Functions
Technologies

Features & Benefits

Labeling Claims

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Stress (Break) ¹¹95MPaISO 527
Tensile Stress (Break) ¹¹97MPaASTM D638
Tensile Strain (Break) ¹¹2.5%ASTM D638
Tensile Strain (Break) ¹¹2.5%ISO 527
Tensile Modulus (at 50 mm/min) ¹¹6890MPaASTM D638
Flexural Stress ¹¹137MPaASTM D790
Flexural Stress ¹¹143MPaISO 178
Flexural Modulus ¹¹6200MPaASTM D790
Flexural Modulus ¹¹6000MPaISO 178
Tensile Modulus (at 1 mm/min) ¹¹6480MPaISO 527
Physical Properties
ValueUnitsTest Method / Conditions
Density ¹¹1.3g/cm³ISO 1183
Density ¹¹1.3g/cm³ASTM D792
Moisture Absorption (at 23°C, 50% RH, 24hrs) ¹¹0.1%ASTM D570
Mold Shrinkage (flow, 24 hrs) ᵍ ¹¹0.41%ISO 294
Mold Shrinkage (flow, 24 hrs) ᵍ ¹¹0.4%ASTM D955
Mold Shrinkage (xflow, 24 hrs) ᵍ ¹¹0.6%ASTM D955
Mold Shrinkage (xflow, 24 hrs) ᵍ ¹¹0.58%ISO 294
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature (at 0.45 MPa, 3.2 mm, Unannealed) ¹¹138°CASTM D648
Heat Deflection Temperature (at 1.82 MPa, 3.2mm, Unannealed) ¹¹135°CASTM D648
Coefficient of Thermal Expansion (at -40°C to 40°C, flow) ¹¹0.00003241/°CASTM E831
Coefficient of Thermal Expansion (at -40°C to 40°C, flow) ¹¹0.0000321/°CISO 11359-2
Coefficient of Thermal Expansion (at -40°C to 40°C, xflow) ¹¹0.00007741/°CASTM E831
Coefficient of Thermal Expansion (at -40°C to 40°C, xflow) ¹¹0.0000771/°CISO 11359-2
Heat Deflection Temperature/Bf (at 0.45 Mpa, Flatw 80*10*4, sp=64mm) ¹¹140°CISO 75/Bf
Heat Deflection Temperature/Af (at 1.8 Mpa, Flatw 80*10*4, sp=64mm) ¹¹134°CISO 75/Af
Impact Properties
ValueUnitsTest Method / Conditions
Izod Impact (Unnotched, at 23°C) ¹¹598J/mASTM D4812
Izod Impact (Notched, at 23°C) ¹¹117J/mASTM D256
Instrumented Dart Impact Energy (Peak, at 23°C) ¹¹18JASTM D3763
Multi-Axial Impact ¹¹5JISO 6603
Izod Impact (Unnotched, 80*10*4, at 23°C) ¹¹37kJ/m²ISO 180/1U
Izod Impact (Notched, 80*10*4, at 23°C) ¹¹11kJ/m²ISO 180/1A
Injection Molding
ValueUnitsTest Method / Conditions
Drying Temperature ⁷80°C
Drying Time ⁷4Hrs
Maximum Moisture Content ⁷0.02%
Melt Temperature ⁷250 - 270°C
Front - Zone 3 Temperature ⁷260 - 270°C
Middle - Zone 2 Temperature ⁷250 - 260°C
Rear - Zone 1 Temperature ⁷230 - 245°C
Mold Temperature ⁷40 - 80°C
Back Pressure ⁷0.2 - 0.3MPa
Screw Speed ⁷30 - 60rpm
Note
  • ᵍ Measurements made from Laboratory test Coupon. Actual shrinkage may vary outside of range due to differences in processing conditions, equipment, part geometry and tool design. It is recommended that mold shrinkage studies be performed with surrogate or legacy tooling prior to cutting tools for new molded article.
  • ⁷ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding.
  • ¹¹ The information stated on Technical Datasheets should be used as indicative only for material selection purposes and not be utilized as specification or used for part or tool design.
 