Polymer Name: Styrenic Thermoplastic Elastomer

Tear Strength: 15.0 - 15.0 kN/m

Strain at Break: 450.0 - 450.0 %

Compression Set (70 °C): 69.0 - 69.0 %

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Chemical Family
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers End Uses

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Breaking Stress8.5MPaISO 527-1
Hardness79Shore ADIN ISO 7619-1
Elongation at Break450%ASTM D 638
Compression Set (23°C)35%ISO 815-1
Compression Set (70°C)69%ISO 815-1
Compression Set (100°C)80%ISO 815-1
Tension at 10% Elongation1.1MPaDIN EN ISO 527-1
Tension at 50% Elongation2.4MPaDIN EN ISO 527-1
Tension at 100% Stretch3.1MPaDIN EN ISO 527-1
Tension at 300% Elongation6.4MPaDIN EN ISO 527-1
Tear Resistance15N/mmISO 34-1
Physical Properties
ValueUnitsTest Method / Conditions
Shrinkage - Flow1.1%ISO 294-4
Shrinkage - Across Flow1.2%ISO 294-4
Density1080kg/m3ISO 1183
Electrical Properties
ValueUnitsTest Method / Conditions
Volume Resistance0.06ohm.mIEC 60093

Regulatory & Compliance