LNP™ THERMOCOMP™ Compound DZ004

1 of 486 products in this brand
LNP THERMOCOMP DZ004 compound is based on Polycarbonate (PC) resin containing 20% milled glass.

Polymer Name: Polycarbonate (PC)

Additives Included: Mold Release Agent

Fillers Included: Glass Fiber, Milled Glass Fiber

Processing Methods: Injection Molding

Flexural Modulus: 3500.0 - 3500.0 MPa

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Chemical Family
Polymer Name
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Flame Rating
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Stress (Break) ¹¹60MPaASTM D638
Tensile Strain (Break) ¹¹4.5%ASTM D638
Tensile Modulus (at 50 mm/min) ¹¹3700MPaASTM D638
Flexural Stress ¹¹96MPaASTM D790
Flexural Modulus ¹¹3500MPaASTM D790
Physical Properties
ValueUnitsTest Method / Conditions
Density ¹¹1.41g/cm³ASTM D792
Mold Shrinkage (flow, 24 hrs) ᵍ ¹¹0.3%ASTM D955
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature (at 1.82 MPa, 3.2mm, Unannealed) ¹¹136°CASTM D648
Relative Temperature Index (Electrical) ᵖ ¹¹125°CUL 746B
Relative Temperature Index (Mechanical with impact) ᵖ ¹¹115°CUL 746B
Relative Temperature Index (Mechanical without impact) ᵖ ¹¹125°CUL 746B
Electrical Properties
ValueUnitsTest Method / Conditions
Hot Wire Ignition (PLC 0) ¹¹min. 1.5mmUL 746A
High Ampere Arc Ignition (PLC 2) ¹¹min. 3mmUL 746A
Volume Resistivity ¹¹40000000000000000 - 59000000000000000Ω.cmASTM D257
High Ampere Arc Ignition (PLC 4) ¹¹min. 1.5mmUL 746A
Surface Resistivity ¹¹30900000000000 - 38700000000000ΩASTM D257
Dielectric Strength (in air, at 1.6mm) ¹¹24.3kV/mmASTM D149
High Voltage Arc Track Rate (PLC) ¹¹4PLC CodeUL 746A
Dissipation Factor (at at 1 MHz) ¹¹0.0083ASTM D150
Impact Properties
ValueUnitsTest Method / Conditions
Izod Impact (Unnotched, at 23°C) ¹¹1142J/mASTM D4812
Izod Impact (Notched, at 23°C) ¹¹58J/mASTM D256
Injection Molding
ValueUnitsTest Method / Conditions
Drying Temperature ⁷120°C
Drying Time ⁷4Hrs
Maximum Moisture Content ⁷0.02%
Melt Temperature ⁷305 - 325°C
Front - Zone 3 Temperature ⁷320 - 330°C
Middle - Zone 2 Temperature ⁷310 - 320°C
Rear - Zone 1 Temperature ⁷295 - 305°C
Mold Temperature ⁷80 - 110°C
Back Pressure ⁷0.2 - 0.3MPa
Screw Speed ⁷30 - 60rpm
Flame Characteristics
ValueUnitsTest Method / Conditions
UL Recognized (94V-1 Flame Class Rating) ᵖmin. 3mmUL 94
UL Recognized (94V-2 Flame Class Rating) ᵖmin. 1.5mmUL 94
Note
  • ᵍ Measurements made from Laboratory test Coupon. Actual shrinkage may vary outside of range due to differences in processing conditions, equipment, part geometry and tool design. It is recommended that mold shrinkage studies be performed with surrogate or legacy tooling prior to cutting tools for new molded article.
  • ᵖ UL ratings shown on the technical datasheet might not cover the full range of thicknesses and colors. For details, please see the UL Yellow Card.
  • ⁷ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding.
  • ¹¹ The information stated on Technical Datasheets should be used as indicative only for material selection purposes and not be utilized as specification or used for part or tool design.
 

Regulatory & Compliance

Certifications & Compliance

Packaging & Availability

Regional Availability
  • Americas
  • Asia
  • North America