Knowde Enhanced TDS
Identification & Functionality
- Chemical Family
- Polymer Name
- Plastics & Elastomers Functions
- Technologies
Features & Benefits
Applications & Uses
- Markets
- Plastics & Elastomers End Uses
- Plastics & Elastomers Processing Methods
Properties
- Flame Rating
- Flame Rating
- IEC 60695-11-10 V0
- Mechanical Properties
- Physical Properties
- Thermal Properties
- Electrical Properties
Value | Units | Test Method / Conditions | |
Elongation Modulus | 3500 | MPa | ISO 527-1 |
Hardness | 85 | Shore D | ASTM D2240 |
Breaking Stress | 100 | MPa | ISO 527-1 |
Elongation at Break | 40 | % | ASTM D 638 |
Charpy Impact Strength (23°C) | 100 | kJ/m2 | STN EN ISO 179 |
Charpy Notched Impact Strength (23°C) | 6 | kJ/m2 | ISO 179/1eA |
Value | Units | Test Method / Conditions | |
Shrinkage - Flow | 1 | % | ISO 294-4 |
Shrinkage - Across Flow | 1.3 | % | ISO 294-4 |
Moisture Absorption (23°C/50%) | 0.07 | % | ISO 62 |
Density | 1300 | kg/m3 | ISO 1183 |
Water Absorption | 0.3 | % | ASTM D570-98 |
Value | Units | Test Method / Conditions | |
Melting Point - DSC (10°C/min) | 343 | °C | ISO 11357-1/-3 |
Continuous Use Temperature | 240 | °C | ISO 2578 |
Heat Deflection Temperature - HDT (1.80 MPa) | 152 | °C | ISO 75-1/-2 |
Coefficient of Thermal Expansion - Flow | 45 | E-6/K | ISO 11359-1/-2 |
Thermal Conductivity (In Tarpaulin) | 0.3 | W/mK | DIN EN 821 |
Thermal Conductivity (Through Tarpaulin) | 0.3 | W/mK | DIN EN 821 |
Fire Behavior (0.8 mm Wall Thickness) | V-0 | - | IEC 60695-11-10 |
Value | Units | Test Method / Conditions | |
Volume Resistance | 100000000000000.0 | ohm.m | IEC 60093 |
Tracking Resistance | 150 | V | IEC 60112 |
Dielectric Strength | 23 | kV/mm | IEC 60243-1 |