WIPELAST TV 10 BK is a black composite material suitable for various automotive market segments. It contains polypropylene-EPDM as the base polymer and 10% talc filler. To achieve optimal processing conditions, it must be pre-dried at 60-100°C in an air-circulating dryer for 2-4 hours, depending on the initial moisture content, to ensure a maximum moisture content of 0.10%. The recommended processing method is injection molding, with a melt temperature range of 200-270°C and a mold temperature range of 20-60°C.

Polymer Name: PP/EPDM

Processing Methods: Injection Molding

Density: 970.0 - 970.0 kg/m³

Strain at Break: 25.0 - 25.0 %

Flexural Modulus: 1100.0 - 1100.0 MPa

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Fillers Included
Polymer Name
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers End Uses
Plastics & Elastomers Processing Methods

Properties

Color
Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus1100.0MPaISO 178
Flexural Strength21.0MPaISO 178
Shore Hardness D (15s)55.0ISO 868
Tensile Modulus1200.0MPaISO 527
Tensile Strength16.0MPaISO 527
Tensile Elongation at Break25.0%ISO 527
Impact Strength (Charpy, at 23°C)no breakkJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)84.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)40.0kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)4.0kJ/m²ISO 179/1eA
Physical Properties
ValueUnitsTest Method / Conditions
Density970.0kg/m³ISO 1183
Global Warming Potential (GWP)0.82kg CO₂ eq.ISO 14040, 14044
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B5054.0°CISO 306
HDT / A (1.8 MPa)54.0°CISO 75-1/-2
HDT / B (0.45 MPa)90.0°CISO 75-1/-2
DSC (Melt Point)164.0°CISO 11357-1/-3
Typical Properties
ValueUnitsTest Method / Conditions
Moisture Contentmax. 0.1%
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Mould Temperature20 - 60°C
Melt Temperature200 - 270°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)14.0cm³/10minISO 1133
Melt Index (MFR)11.0g/10minISO 1133
MVR Temperature230.0°C
MVR Load2.16kg
Molding Shrinkage (parallel)1.2%ISO 294-4, 2577
Molding Shrinkage (normal)0.8%ISO 294-4, 2577

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • 60-100°C in an air circulating dryer for 2-4h
  • Dependant on moisture content

Storage & Handling

Storage Conditions

Store in dry, protected from light.