MOCOM Compounds ALCOM® LB ABS 1000 15018 WT1029-15 is a pre-dried acrylonitrile/butadiene/styrene/copolymer containing a special filler, designed for highly reflective and opaque automotive and lighting components such as light guides and reflectors. It should be processed with a melt temperature of 220-260°C and a mold temperature of 50-80°C. The maximum moisture content should not exceed 0.02%.

Polymer Name: Acrylonitrile Butadiene Styrene (ABS)

Fillers Included: Mineral, Proprietary

Processing Methods: Injection Molding

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Fillers Included
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus2600.0MPaISO 178
Flexural Stress (3.5% Strain)73.0MPaISO 178
Tensile Modulus2400.0MPaISO 527
Tensile Stress at Yield49.0MPaISO 527
Tensile Elongation at Yield2.9%ISO 527
Tensile Elongation at Break11.0%ISO 527
Impact Strength (Charpy, at 23°C)175.0kJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)95.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)15.0kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)5.0kJ/m²ISO 179/1eA
Ball Indentation Hardness (H358/30)100.0MPaISO 2039-1
Physical Properties
ValueUnitsTest Method / Conditions
Density1090.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B50106.0°CISO 306
HDT / A (1.8 MPa)91.0°CISO 75-1/-2
Typical Properties
ValueUnitsTest Method / Conditions
Moisture Contentmax. 0.02%
Optical Properties
ValueUnitsTest Method / Conditions
Tristimulus Value Y10 of Reflection68.0%DIN 5033
Tristimulus Value Y10 of Transm.,d=0.5mm0.1%ISO 13468
Flammability
ValueUnitsTest Method / Conditions
Glow Wire (GWFI, 650°C, 1mm)PassedDIN EN 60695
Glow Wire (GWFI, 650°C, 2mm)PassedDIN EN 60695
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Melt Temperature220 - 260°C
Mould Temperature50 - 80°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)5.0cm³/10minISO 1133
MVR Temperature220.0°C
MVR Load10.0kg
Shrinkage (24h)0.5 - 0.8%ISO 294-4

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • 80 °C in a dry air (dessiccant) dryer for 2-4 h
  • 80 °C in an air circulating dryer for 4-8 h

Storage & Handling

Storage Conditions

Store in dry, protected from light.