company tower banner
MOCOM Compounds Company Logo

CELLIDOR® CP 300-10

1 of 27 products in this brand
MOCOM Compounds CELLIDOR® CP 300-10 is a base polymer composed of cellulose acetate propionate, with a 10% phthalate-free plasticiser. It is suitable for use in the production of toothbrushes and other products. It should be pre-dried in an air circulating dryer at temperatures between 60-90°C for 2-4 hours, depending on the moisture content. For injection molding, the melt temperature should be between 180-230°C and the mold temperature should be between 40-80°C. No extra sentence required.

Polymer Name: Cellulose Acetate Propionate (CAP)

Additives Included: Plasticizer (Phthalate-free)

Density: 1200.0 - 1200.0 kg/m³

End Uses: Hearing Aid, Toothbrushes

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Plastics & Elastomers Functions
Technologies

Features & Benefits

Materials Features

Applications & Uses

Plastics & Elastomers End Uses
Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus1900.0MPaISO 178
Flexural Stress (3.5% Strain)50.0MPaISO 178
Tensile Modulus1950.0MPaISO 527
Tensile Stress at Yield45.0MPaISO 527
Tensile Elongation at Yield4.1%ISO 527
Tensile Elongation at Break15.0%ISO 527
Impact Strength (Charpy, at 23°C)190.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)20.0kJ/m²ISO 179/1eA
Ball Indentation Hardness (H358/30)65.0MPaISO 2039-1
Physical Properties
ValueUnitsTest Method / Conditions
Density1200.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B5096.0°CISO 306
HDT / A (1.8 MPa)92.0°CISO 75-1/-2
Typical Properties
ValueUnitsTest Method / Conditions
Moisture Contentmax. 0.15%
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Melt Temperature180 - 230°C
Mould Temperature40 - 80°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)5.0cm³/10minISO 1133
MVR Temperature210.0°C
MVR Load2.16kg
Shrinkage (24h)0.7 - 0.9%ISO 294-4

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • In an air circulatIng dryer 60-90 °C for 2-4 h
  • Dependant on moisture content

Storage & Handling

Storage Conditions

Store in dry, protected from light not above 30°C.