MOCOM Compounds CELLIDOR® CP 430-13 AG is a base polymer composed of Cellulose Acetate Propionate with 13% phthalate-free plasticiser. Pre-drying conditions require an air circulating dryer with a temperature between 50-80°C for 2-4 h, depending on moisture content, with a maximum moisture content of less than 0.05%. For processing injection molding, an extrusion melt temperature of 180-230°C and an indie temperature of 40-80°C are required.

Polymer Name: Cellulose Acetate Propionate (CAP)

Additives Included: Plasticizer (Phthalate-free)

Density: 1200.0 - 1200.0 kg/m³

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Plastics & Elastomers Functions
Technologies

Features & Benefits

Materials Features

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus1600.0MPaISO 178
Flexural Stress (3.5% Strain)45.0MPaISO 178
Tensile Modulus1500.0MPaISO 527
Tensile Stress at Yield34.0MPaISO 527
Tensile Elongation at Yield3.7%ISO 527
Tensile Elongation at Break19.0%ISO 527
Impact Strength (Charpy, at 23°C)no breakkJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)220.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)30.0kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)7.0kJ/m²ISO 179/1eA
Ball Indentation Hardness (H132/30)75.0MPaISO 2039-1
Physical Properties
ValueUnitsTest Method / Conditions
Density1200.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B5086.0°CISO 306
HDT / A (1.8 MPa)82.0°CISO 75-1/-2
Typical Properties
ValueUnitsTest Method / Conditions
Moisture Contentmax. 0.05%
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Extrusion Melt Temperature180 - 230°C
Die Temperature40 - 80°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)9.0cm³/10minISO 1133
MVR Temperature210.0°C
MVR Load2.16kg
Shrinkage (24h)0.4 - 0.7%ISO 294-4

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • In an air circulatIng dryer 50-80 °C for 2-4 h
  • Dependant on moisture content

Storage & Handling

Storage Conditions

Store in dry, protected from light not above 30°C.