MOCOM Compounds ALTECH® ABS A 3230/516 GK20 GF10 is a black, impact-modified, high-stiffness, and processing-stabilized acrylonitrile/butadiene/styrene/copolymer containing 30% glass fibers/glass beads. For injection molding, the suggested melt temperature is between 220-260°C and the mold temperature should be between 50-80°C. This material is suitable for various injection-molded parts and has numerous applications in multiple market segments.

Polymer Name: Acrylonitrile Butadiene Styrene (ABS)

Fillers Included: Glass Bead, Glass Bead/Glass Fiber

Functions: Resin

Chemical Family: Acrylonitrile Butadiene Styrene (ABS), Styrenics

Processing Methods: Injection Molding

Additives Included: Impact Modifier, Processing Stabilizer

Features: Heat Aging Resistant, High Stiffness, Impact Modified, Processing Stability

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Color
Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus4000.0MPaISO 178
Flexural Strength62.0MPaISO 178
Tensile Modulus3300.0MPaISO 527
Tensile Strength at Break39.0MPaISO 527
Tensile Elongation at Break1.7%ISO 527
Impact Strength (Charpy, at 23°C)13.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)4.5kJ/m²ISO 179/1eA
Ball Indentation Hardness (H358/30)97.0MPaISO 2039-1
Physical Properties
ValueUnitsTest Method / Conditions
Density1260.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B5093.0°CISO 306
HDT / A (1.8 MPa)85.0°CISO 75-1/-2
Typical Properties
ValueUnitsTest Method / Conditions
Moisture Contentmax. 0.2%
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Melt Temperature220 - 260°C
Mould Temperature50 - 80°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)11.0cm³/10minISO 1133
MVR Temperature220.0°C
MVR Load10.0kg
Shrinkage (Lengthwise, 24h)0.2 - 0.4%ISO 294-4
Shrinkage (Lateral, 24h)0.3 - 0.5%ISO 294-4

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • 80 °C in a dry air (dessiccant) dryer for 2-4 h
  • 80 °C in an air circulating dryer for 3-6 h
  • Dependant on moisture content

Storage & Handling

Storage Conditions

Store in dry, protected from light not above 30°C.