MOCOM Compounds ALTECH® PP-H B 2012/500 GF12 is a Polypropylene Homopolymer pre-dried in an air circulating dryer or in a dry air (dessiccant) dryer. The melt temperature for processing injection molding is 200-250°C and the mold temperature is 20-70°C. The filler/additive system is 12% glass fibers, chemically coupled, heat stabilized, with an easy release (demolding) and slip agent. The market segment for this material is Furniture, building and construction, sport and leisure, and various. The application area is for household goods and domestic appliances and the typical applications are furniture profile and racking/shelving.

Polymer Name: Polypropylene Homopolymer (HPP)

Processing Methods: Injection Molding

Additives Included: Heat Stabilizer, Slip Agent

Fillers Included: Glass Fiber

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Fillers Included
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus2600.0MPaISO 178
Flexural Strength80.0MPaISO 178
Tensile Modulus2800.0MPaISO 527
Tensile Strength at Break50.0MPaISO 527
Tensile Elongation at Break4.0%ISO 527
Impact Strength (Charpy, at 23°C)40.0kJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)25.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)10.0kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)6.0kJ/m²ISO 179/1eA
Physical Properties
ValueUnitsTest Method / Conditions
Density970.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B50116.0°CISO 306
HDT / A (1.8 MPa)130.0°CISO 75-1/-2
DSC (Melt Point)166.0°CISO 11357
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Mould Temperature20 - 70°C
Melt Temperature200 - 250°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)13.0cm³/10minISO 1133
MVR Temperature230.0°C
MVR Load2.16kg
Shrinkage (Lengthwise, 24h)0.5 - 0.7%ISO 294-4
Shrinkage (Lateral, 24h)0.5 - 0.7%ISO 294-4

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • In a dry air (dessiccant) dryer 80-120 °C for 2-3 h
  • In an air circulatIng dryer 80-120 °C for 2-4 h

Storage & Handling