MOCOM Compounds ALCOM® AWL 15/1 WT31-956LB is a pre-dried acrylonitrile/butadiene/styrene/copolymer that contains a 15% special filler system, designed for automotive and various applications such as lighting and light blocking components, like light guides and reflectors. It has a high reflectivity and opacity. For injection molding, a melt temperature of 220-260°C and a mold temperature of 50-80°C should be used, and the maximum moisture content should not exceed 0.02%.

Polymer Name: Acrylonitrile Butadiene Styrene (ABS)

Fillers Included: Proprietary

Processing Methods: Injection Molding

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Fillers Included
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus2800.0MPaISO 178
Flexural Stress (3.5% Strain)75.0MPaISO 178
Tensile Modulus2900.0MPaISO 527
Tensile Stress at Yield50.0MPaISO 527
Tensile Elongation at Yield2.8%ISO 527
Tensile Elongation at Break12.0%ISO 527
Impact Strength (Charpy, at 23°C)70.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)9.0kJ/m²ISO 179/1eA
Ball Indentation Hardness (H358/30)120.0MPaISO 2039-1
Ball Indentation Temperature106.0°CDIN EN 60695-10-2
Physical Properties
ValueUnitsTest Method / Conditions
Density1170.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B50110.0°CISO 306
HDT / A (1.8 MPa)93.0°CISO 75-1/-2
Typical Properties
ValueUnitsTest Method / Conditions
Moisture Contentmax. 0.02%
Optical Properties
ValueUnitsTest Method / Conditions
Tristimulus Value Y10 of Reflection93.0%DIN 5033
Tristimulus Value Y10 of Transm.,d=0.5mm0.4%ISO 13468
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Melt Temperature220 - 260°C
Mould Temperature50 - 80°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)5.0cm³/10minISO 1133
MVR Temperature220.0°C
MVR Load10.0kg
Shrinkage (24h)min. 0.45%ISO 294-4

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • 80 °C in a dry air (dessiccant) dryer for 2-4 h
  • 80 °C in an air circulating dryer for 4-8 h

Storage & Handling

Storage Conditions

Store in dry, protected from light.