MOCOM Compounds Company Logo

ALCOM® PP 620/1 MR40 WT1034-05LB

1 of 363 products in this brand
MOCOM Compounds ALCOM® PP 620/1 MR40 WT1034-05LB is a polypropylene homopolymer pre-dried using a dry air (dessiccant) dryer or an air circulating dryer at 80-100°C for 2-4 hours, with a maximum moisture content of <0.02%. It features 40% special filler, providing a highly reflective, opaque material. It is commonly used for light guides, reflectors, and light blocking components in the automotive and lighting markets. It is processed through injection molding with a melt temperature of 230-270°C and a mold temperature of 20-90°C.

Polymer Name: Polypropylene Homopolymer (HPP)

Processing Methods: Injection Molding

Functions: Resin

Fillers Included: Mineral, Proprietary

Labeling Claims: Azo Colorants-free, Azo Dyes-free, Conflict minerals-free, PAH-free, PFOA-free, PFOS-free, Persistent Organic Pollutants (POP)-free

End Uses: Automotive Applications, Automotive Exterior Parts, Light Blocking Components, Light Guides, Reflectors

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Fillers Included
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus3600.0MPaISO 178
Flexural Stress (3.5% Strain)50.0MPaISO 178
Tensile Modulus3200.0MPaISO 527
Tensile Stress at Yield29.0MPaISO 527
Tensile Elongation at Yield2.6%ISO 527
Tensile Elongation at Break4.0%ISO 527
Impact Strength (Charpy, at 23°C)28.0kJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)10.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)2.5kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)1.5kJ/m²ISO 179/1eA
Physical Properties
ValueUnitsTest Method / Conditions
Density1270.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B50102.0°CISO 306
HDT / A (1.8 MPa)85.0°CISO 75-1/-2
DSC (Melt Point)163.0°CISO 11357
Typical Properties
ValueUnitsTest Method / Conditions
Moisture Contentmax. 0.02%
Optical Properties
ValueUnitsTest Method / Conditions
Tristimulus Value Y10 of Reflection94.0%DIN 5033
Tristimulus Value Y10 of Transm.,d=0.5mm0.2%ISO 13468
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Mould Temperature20 - 90°C
Melt Temperature230 - 270°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)22.0cm³/10minISO 1133
MVR Temperature230.0°C
MVR Load2.16kg
Shrinkage (Lengthwise, 24h)0.9 - 1.1%ISO 294-4
Shrinkage (Lateral, 24h)1 - 1.2%ISO 294-4

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • In a dry air (dessiccant) dryer 80-100 °C for 2-3 h
  • In an air circulatIng dryer 80-100 °C for 2-4 h

Storage & Handling

Storage Conditions

Store in dry, protected from light.