company tower banner
MOCOM Compounds Company Logo

ALCOM® AWL 109/15 WT1217-11LB

1 of 363 products in this brand
MOCOM Compounds ALCOM® AWL 109/15 WT1217-11LB is a highly reflective, opaque, and high heat stabilized Acrylonitrile/Butadiene/Styrene/Copolymer modified with polycarbonate and 15% special filler. It is used in automotive, various lighting, and light blocking components and its typical applications are light guides and reflectors. It is approved by GMW15702 and should be processed with a melt temperature of 230-270°C and a mold temperature of 60-100°C.

Polymer Name: PC/ABS Alloy

Processing Methods: Injection Molding

Density: 1240.0 - 1240.0 kg/m³

Flexural Modulus: 2700.0 - 2700.0 MPa

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Fillers Included
Polymer Name
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus2700.0MPaISO 178
Flexural Strength75.0MPaISO 178
Tensile Modulus2700.0MPaISO 527
Tensile Stress at Yield50.0MPaISO 527
Tensile Elongation at Yield3.0%ISO 527
Tensile Elongation at Break13.0%ISO 527
Impact Strength (Charpy, at 23°C)85.0kJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)83.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)13.0kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)8.0kJ/m²ISO 179/1eA
Ball Indentation Hardness (H358/30)115.0MPaISO 2039-1
Ball Indentation Temperature100.0°CDIN EN 60695-10-2
Physical Properties
ValueUnitsTest Method / Conditions
Density1240.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B50110.0°CISO 306
HDT / A (1.8 MPa)100.0°CISO 75-1/-2
Typical Properties
ValueUnitsTest Method / Conditions
Moisture Contentmax. 0.02%
Optical Properties
ValueUnitsTest Method / Conditions
Tristimulus Value Y10 of Reflection93.0%DIN 5033
Tristimulus Value Y10 of Transm.,d=0.5mm0.4%ISO 13468
Flammability
ValueUnitsTest Method / Conditions
Flammability (1.5 mm)HBclassUL 94
Flammability (3.0 mm)HBclassUL 94
UL Recognitionyes
Yellow Card Availableyes
Glow Wire (GWFI, 650°C, 1mm)PassedDIN EN 60695
Glow Wire (GWFI, 650°C, 2mm)PassedDIN EN 60695
Glow Wire (GWFI, 650°C, 3mm)PassedDIN EN 60695
Fire Behavior FMVSS (2.0 mm)PassedFMVSS 302/DIN 75200
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Melt Temperature230 - 270°C
Mould Temperature60 - 100°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)15.0cm³/10minISO 1133
MVR Temperature220.0°C
MVR Load10.0kg
Shrinkage (24h)0.4 - 0.7%ISO 294-4

Regulatory & Compliance

OEM Specifications

Technical Details & Test Data

Pre-Drying Conditions
  • In a dry air (dessiccant) dryer 80-90 °C for 2-4 h
  • In an air circulatIng dryer 80-90 °C for 4-8 h

Storage & Handling

Storage Conditions

Store in dry, protected from light.