MOCOM Compounds ALFATER® XL A70I 3EFSL0000 is a thermoplastic vulcanisate (PP+EPDM) polymer suitable for injection molding. It has improved abrasion resistance, slip-optimized, easy flow, high surface quality, good weathering resistance, good chemical resistance, good ozone resistance, good hot air resistance, and good hydrolysis resistance. It is suitable for automotive, building and construction, electrical and electronic, sport and leisure, and furniture applications and can be used for injection molded parts such as seals, sealing lip, handles, soft touch elements, impact protection/shock absorber, bearings and sliding elements, thin walled parts, profile, cable ducts, 2K components, and casters. It has good adhesion to various polymers and has a service temperature range of -40-125°C. The polymer should be stored dry, protected from light, at a temperature not exceeding 30°C, and tightly sealed.

Polymer Name: PP/EPDM

Processing Methods: Injection Molding

Labeling Claims: Azo Colorants-free, Azo Dyes-free, Conflict minerals-free, PAH-free, PFOA-free, PFOS-free, Persistent Organic Pollutants (POP)-free

Density: 950.0 - 950.0 kg/m³

Tear Strength: 23.0 - 23.0 kN/m

Features: Abrasion Resistant, Chemical Resistant, Excellent Hydrolysis Resistance, Flexible, Good Flow, Good Weather Stability, Hot Air Resistant, Ozone Resistant, Slip-Optimized, Soft, Soft Touch, Superior Surface Quality

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Fillers Included
Polymer Name
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Color
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength (Type 2)5.0MPaISO 37
Tear Strength (Method Ba)23.0kN/mISO 34-1
Elongation at Break (Type 2)400.0%ISO 37
Shore Hardness A (15s)70.0ISO 868
Tensile Stress at 100% Elongation (Type 2)2.8MPaISO 37
Physical Properties
ValueUnitsTest Method / Conditions
Density950.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Compression Set (22h, at 70°C, 25%, Type A)35.0%ISO 815
Compression Set (22h, at 100°C, 25%, Type A)43.0%ISO 815
Compression Set (72h, at 22°C, 25%, Type A)23.0%ISO 815
Compression Set (72h, at 125°C, 25%, Type A)54.0%ISO 815
Typical Properties
ValueUnitsTest Method / Conditions
Service Temperature (depending on load, geometry, etc.)- 40 to 125°C
Moisture Contentmax. 0.1%
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Back Pressure (hydraulic)min. 3bar
Mould Temperature10 - 60°C
Melt Temperature190 - 220°C
Holding Pressure (of injection pressure)50 - 70%
Injection SpeedMiddle - High
Tribological Properties
ValueUnitsTest Method / Conditions
Abrasion (Method A)260.0mm³ISO 4649
Rheological Properties
ValueUnitsTest Method / Conditions
Shrinkage (Lengthwise, 24h)1.3 - 1.7%ISO 294-4
Shrinkage (Lateral, 24h)0.9 - 1.3%ISO 294-4
Spiral Flow (2 mm wall thickness)110.0cm

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions

In a dry air (dessiccant) dryer 70-80 °C for 2-4 h

Storage & Handling

Storage Conditions