MOCOM Compounds ALCOM® LB ECO PC+ABS 1000 SL WT1023-21 is a pre-dried injection molding grade with a polycarbonate + acrylonitrile butadiene styrene blend. It is highly reflective, contains recycled material, has anti-squeak modifications, and is opaque. It is used in the automotive, electrical and electronic, and lighting markets and is typically used for light guides and reflectors. When processing injection molding, the melt temperature should be 240-280°C and the mold temperature should be 70-100°C.

Polymer Name: PC/ABS Alloy

Processing Methods: Injection Molding

Density: 1260.0 - 1260.0 kg/m³

Flexural Modulus: 2000.0 - 2000.0 MPa

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Polymer Name
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus2000.0MPaISO 178
Flexural Stress (3.5% Strain)60.0MPaISO 178
Tensile Modulus2000.0MPaISO 527
Tensile Stress at Yield42.0MPaISO 527
Tensile Elongation at Yield3.3%ISO 527
Tensile Elongation at Break75.0%ISO 527
Impact Strength (Charpy, at 23°C)255.0kJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)220.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)65.0kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)7.0kJ/m²ISO 179/1eA
Ball Indentation Hardness (H358/30)83.0MPaISO 2039-1
Physical Properties
ValueUnitsTest Method / Conditions
Density1260.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B50104.0°CISO 306
HDT / A (1.8 MPa)99.0°CISO 75-1/-2
Optical Properties
ValueUnitsTest Method / Conditions
Tristimulus Value Y10 of Reflection93.0%DIN 5033
Total Transmission T(Y) (d=2,0mm, A, 2°)0.0%ISO 13468
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Melt Temperature240 - 280°C
Mould Temperature70 - 100°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)17.0cm³/10minISO 1133
MVR Temperature260.0°C
MVR Load5.0kg
Shrinkage (24h)0.6 - 0.8%ISO 294-4

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • In a dry air (dessiccant) dryer 100-110 °C for 2-4 h
  • In an air circulatIng dryer 100-110 °C for 3-6 h

Storage & Handling

Storage Conditions

Store in dry, protected from light.