MOCOM Compounds ALCOM® LB PC+ABS 1000 19037 RD1036-19 is an injection molding grade polymer blend of polycarbonate and Acrylonitrile Butadiene Styrene that is highly reflective and opaque. It is used in automotive, electrical and electronic, and lighting market segments for applications such as light guides and reflectors. During processing injection molding, a melt temperature of 250-280°C and mold temperature of 70-100°C should be maintained. After processing, the material should be stored in a dark environment to protect it from light.

Polymer Name: PC/ABS Alloy

Processing Methods: Injection Molding

Density: 1160.0 - 1160.0 kg/m³

Flexural Modulus: 2400.0 - 2400.0 MPa

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Polymer Name
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus2400.0MPaISO 178
Flexural Stress (3.5% Strain)73.0MPaISO 178
Tensile Modulus2400.0MPaISO 527
Tensile Stress at Yield53.0MPaISO 527
Tensile Elongation at Yield4.2%ISO 527
Tensile Elongation at Break40.0%ISO 527
Impact Strength (Charpy, at 23°C)no breakkJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)no breakkJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)42.0kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)18.0kJ/m²ISO 179/1eA
Physical Properties
ValueUnitsTest Method / Conditions
Density1160.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B50125.0°CISO 306
HDT / A (1.8 MPa)108.0°CISO 75-1/-2
Typical Properties
ValueUnitsTest Method / Conditions
Moisture Contentmax. 0.02%
Optical Properties
ValueUnitsTest Method / Conditions
Tristimulus Value Y10 of Reflection16.0%DIN 5033
Tristimulus Value Y10 of Transm.,d=0.5mm0.4%ISO 13468
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Melt Temperature250 - 280°C
Mould Temperature70 - 100°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)25.0cm³/10minISO 1133
MVR Temperature260.0°C
MVR Load5.0kg
Shrinkage (24h)0.6 - 0.8%ISO 294-4

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • In a dry air (dessiccant) dryer 100-110 °C for 2-4 h
  • In an air circulatIng dryer 100-110 °C for 4-8 h

Storage & Handling

Storage Conditions

Store in dry, protected from light.