MOCOM Compounds ALTECH® PP-H A 2440/550 GF25 MR15 CP is a polypropylene homopolymer with 25% glass fibers and 15% talcum pre-dried in a dry air (dessiccant) dryer at 80-120°C for 2-3 hours or an air circulating dryer at 80-120°C for 2-4 hours, with a melt temperature of 200-250°C and a mold temperature of 20-70°C. It is high heat stabilized, chemically coupled, and has high stiffness and easy release (demolding). It is suitable for automotive, electrical, and electronic applications such as exterior parts, interior decoration/finishing, electrical components, and injection molded parts.

Polymer Name: Polypropylene Homopolymer (HPP)

Processing Methods: Injection Molding

Additives Included: Heat Stabilizer

Fillers Included: Glass Fiber, Mineral, Talc

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Fillers Included
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus7600.0MPaISO 178
Flexural Strength130.0MPaISO 178
Tensile Modulus8000.0MPaISO 527
Tensile Strength at Break85.0MPaISO 527
Tensile Elongation at Break2.7%ISO 527
Impact Strength (Charpy, at 23°C)40.0kJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)30.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)8.0kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)6.0kJ/m²ISO 179/1eA
Physical Properties
ValueUnitsTest Method / Conditions
Density1220.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B50144.0°CISO 306
HDT / A (1.8 MPa)155.0°CISO 75-1/-2
DSC (Melt Point)163.0°CISO 11357
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Mould Temperature20 - 70°C
Melt Temperature200 - 250°C
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)6.0cm³/10minISO 1133
MVR Temperature230.0°C
MVR Load2.16kg
Shrinkage (Lengthwise, 24h)0.3 - 0.5%ISO 294-4
Shrinkage (Lateral, 24h)0.5 - 0.7%ISO 294-4

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • In a dry air (dessiccant) dryer 80-120 °C for 2-3 h
  • In an air circulatIng dryer 80-120 °C for 2-4 h

Storage & Handling

Storage Conditions

Store in dry, protected from light not above 30°C.