Knowde Enhanced TDS
Identification & Functionality
- Additives Included
- Polymer Name
- Plastics & Elastomers Functions
- Technologies
- Product Families
Features & Benefits
- Labeling Claims
- Materials Features
Applications & Uses
- Applications
- Plastics & Elastomers End Uses
- Plastics & Elastomers Processing Methods
Properties
- Mechanical Properties
- Physical Properties
- Thermal Properties
- Flammability
- Processing Information (Injection Molding)
- Rheological Properties
Value | Units | Test Method / Conditions | |
Flexural Modulus | 2600.0 | MPa | ISO 178 |
Flexural Strength | 75.0 | MPa | ISO 178 |
Tensile Modulus | 2450.0 | MPa | ISO 527 |
Tensile Strength | 45.0 | MPa | ISO 527 |
Tensile Elongation at Break | 8.0 | % | ISO 527 |
Impact Strength (Charpy, at 23°C) | 90.0 | kJ/m² | ISO 179/1eU |
Notched Impact Strength (Charpy, at 23°C) | 20.0 | kJ/m² | ISO 179/1eA |
Value | Units | Test Method / Conditions | |
Density | 1190.0 | kg/m³ | ISO 1183 |
Value | Units | Test Method / Conditions | |
Vicat B50 | 119.0 | °C | ISO 306 |
HDT / A (1.8 MPa) | 105.0 | °C | ISO 75-1/-2 |
Value | Units | Test Method / Conditions | |
Flammability (1.5 mm) | HB | class | UL 94 |
Value | Units | Test Method / Conditions | |
Melt Temperature | 260 - 300 | °C | — |
Mould Temperature | 60 - 90 | °C | — |
Value | Units | Test Method / Conditions | |
Melt Index (MVR) | 18.0 | cm³/10min | ISO 1133 |
MVR Temperature | 260.0 | °C | — |
MVR Load | 5.0 | kg | — |
Shrinkage (24h) | 0.4 - 0.7 | % | ISO 294-4 |
Regulatory & Compliance
Technical Details & Test Data
- Pre-Drying Conditions
- In a dry air (dessiccant) dryer 90-110 °C for 2-4 h
- In an air circulatIng dryer 90-110 °C for 4-8 h
- Dependant on moisture content
Storage & Handling
- Storage Conditions
Store in dry, protected from light.